at what angle would the tapered hole be in a hammer head.....eg a medium size ball pein with wooden handle?
-
1st Apr 2018, 12:23 PM #2
-
1st Apr 2018, 12:35 PM #3
Shouldn’t a ball pien hammer have a hour glass eye? Tapered from both sides. That’s how we are taught to Forge hammers.
…..Live a Quiet Life & Work with your Hands
-
1st Apr 2018, 12:40 PM #4
-
1st Apr 2018, 07:27 PM #5Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,562
I vaguely remember my father replacing a handle (Claw hammer?) and filing/ rasping it to fit. I suspect that older hammers were what the manufacturer said they were and handles shaped to fit.
Michael
-
1st Apr 2018, 07:48 PM #6
I worked in the building industry for many years, the hammer handles you buy are alway to large, so you need to rasp them down and use wedges. Usually the handle is worth more than half a decent hammer, so you just buy a new hammer to save the hassle. The new hammers seem to come with some sort of resin over the wedge.
Using Tapatalk
-
1st Apr 2018, 09:15 PM #7
https://www.anvilfire.com/FAQs/hamme...dimensions.htm
Tapered sledge eyes taper to center 4° on long axis and 3° on short axis. This is for punches and finished holes.…..Live a Quiet Life & Work with your Hands
Similar Threads
-
Indexing head or dividing head?
By stevee7270 in forum METALWORK GENERALReplies: 16Last Post: 16th May 2016, 03:13 PM -
Indexing head or dividing head?
By stevee7270 in forum METALWORK GENERALReplies: 1Last Post: 26th Apr 2016, 04:34 PM -
a hammer
By eskimo in forum METALWORK GENERALReplies: 8Last Post: 22nd Feb 2015, 05:35 PM -
trip hammer
By Marc in forum THE SMITHYReplies: 16Last Post: 3rd Nov 2014, 11:18 AM -
How big a hammer do you need?
By Michael G in forum METALWORK GENERALReplies: 31Last Post: 24th Nov 2012, 06:22 PM