Modifying Vincent HRD Rapide motorcycle drive shafts.
This modification adds an oil seal to the end of the drive shaft to eliminate one of the sources of oil leakage.<br>
These shaft are case hardened and required a tungsten carbide insert to rough out most of the material and a finishing insert to achieve the final size and finish.
-
17th Jan 2018, 11:19 AM #2Banned
- Join Date
- Feb 2015
- Location
- Oz
- Age
- 73
- Posts
- 459
You have a Vincent, what model?
Attachments aren't working BTW.
-
17th Jan 2018, 02:52 PM #3
What’s the point of a pommy bike without oil leaks.
I saw one the new Egli Swiss manufactured motors recently,what impressed me most was the starter motor.
About $30k apparently.
The top spine of the frame was a cnc machined oil tank.
Just how oil tight it’ll stay with the mono shock anchored to the rear of it remains to be seen.
I’d post pics but if I did I’d have to kill you all.
H.Jimcracks for the rich and/or wealthy. (aka GKB '88)
-
17th Jan 2018, 09:04 PM #4.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,459
P1050339.jpg
Something like this H? A Terry Prince and Fritz Egli Junior creation. More here - TPV Vincent Start » TPV VincentLast edited by Anorak Bob; 18th Jan 2018 at 10:01 AM. Reason: Credit and link added for those who may be interested.
-
17th Jan 2018, 09:19 PM #5Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
That's pretty much like the standard Vincent arrangement, minus triangulation of the swinging arm.
-
17th Jan 2018, 10:03 PM #6Golden Member
- Join Date
- Sep 2008
- Location
- Riddells Creek, Vic.
- Posts
- 838
-
20th Jan 2018, 02:02 AM #7Banned
- Join Date
- Feb 2015
- Location
- Oz
- Age
- 73
- Posts
- 459
Yep, they are. If ever a machine was described as beautiful, surely the Vincent engine was it. Left arm stuff!
-
20th Jan 2018, 07:06 AM #8Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
An unusual aspect of Vincent's design compared to most motorbike engines is the rocker pivot shafts that aren't parallel to the crankshaft.
They are more similar to how aero radial engines have their rocker gear laid out, and gives the cylinder heads a distinctive look.
Jordan
Similar Threads
-
Modifying a Wohlhaupter UPA4.
By LexD in forum METALWORK PROJECTSReplies: 42Last Post: 9th Dec 2017, 08:12 AM -
Motorcycle bar end form tool
By welder in forum METALWORK GENERALReplies: 4Last Post: 23rd Mar 2016, 08:28 PM -
Low Height Motorcycle Trailer
By Wood66 in forum TRAILERS & OTHER FABRICATED STUFFReplies: 44Last Post: 23rd Dec 2012, 01:53 PM -
Intro & Motorcycle trailer
By Chexfxdx in forum TRAILERS & OTHER FABRICATED STUFFReplies: 6Last Post: 16th Apr 2012, 06:55 PM -
Modifying a caravan to a flat bed
By Chooks74 in forum TRAILERS & OTHER FABRICATED STUFFReplies: 9Last Post: 27th Jan 2009, 05:25 PM