Good carbide end mill source?
I had some spring steel recently (HRC up to 63 according to wikipedia) and it ate my HSS cutters - 3 in fact.
So I was thinking I'd buy a carbide end mill set to cut harder materials. Anyone have a good source, like on ebay for a set? I found a few single ones but they stated they'd cut up to HRC 45 which seems too low, e.g. https://www.ebay.com.au/itm/12mm-dia...8AAOSw0GJZpNh-
Are these any good? https://www.ebay.com.au/itm/5Pcs-Tun...AAAOSwvYZZmqs5
Cheers
-
4th Jan 2018, 01:59 PM #2Senior Member
- Join Date
- Oct 2009
- Location
- Upwey VIC
- Posts
- 187
https://www.lprtoolmakers.com.au/car...ank-2-to-12mm/
Haven't tried them myself, yet.
Andrew
-
4th Jan 2018, 06:19 PM #3Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,038
I've used these Wenling guys on AliExpress for lathe and mill tooling and have been well satisfied YMMV. I haven't tried any of their end mills but I see they offer carbide end mills up to 60HRC.
https://www.aliexpress.com/store/gro...477e8752TkX2yu
Looking at the ebay store attached to your link I don't think the seller has much metal machining expertise.
-
5th Jan 2018, 01:58 PM #4Novice
- Join Date
- May 2011
- Location
- Albury
- Posts
- 11
I'm afraid you generally get what you pay for when it comes to carbide tooling. Tools suitable for use on materials up to HRC45 are a common starting hardness. Tools to handle material up to HRC65 are generally available. Coatings and grind can make a considerable difference to tool life and suitability for purpose.
Have a look at this - https://www.youtube.com/watch?v=nY6o04ODJ3U
-
5th Jan 2018, 06:17 PM #5Most Valued Member
- Join Date
- Oct 2007
- Location
- Sydney
- Posts
- 3,112
I’ve used this seller reasonably often for carbide tools over the years. Items in carbidechiu store on eBay !
While carbide is definitely NOT all the same (as was suggested by a forum member recently), by the same token it can be taken to be more complex than may be required for most of us here. My experience is that a tool running under CNC control on a rigid machine will be run harder and more towards its highest optimum cutting ability when compared to manual use. So while the talk of coatings and higher grades of carbide are definitely true, I don’t think it’s worth losing too much sleep over as long as you’re running the tool somewhat close to its intended purpose. The recent discussion questioning (quite rudely) why a masonry drill wasn’t “just the same” as a drill designed for drilling multiple materials would be an example. A carbide end mill designed for cutting aluminium is probably not going to hold up well to heavy interrupted cuts in hardened steel, so that would be another example. Etc etc.
For onsies-twosies I wouldn’t fuss over it too much, and I’ve never had any issues with the tooling from the above supplier.
-
5th Jan 2018, 08:15 PM #6Senior Member
- Join Date
- Jun 2005
- Location
- Townsville, Tropical Nth Qld.
- Posts
- 225
Up above in the Your favorite tooling supplier thread, Toggy said he bought some from Maritool. I checked the site but was not exactly sure which ones he bought.
Rgds,
Crocy
-
6th Jan 2018, 06:55 AM #7Golden Member
- Join Date
- Jun 2004
- Location
- Kyabram. Vic
- Posts
- 632
That was me.
I went for the variable flute variety. Got the set plus an extra 5/8".
Very nice looking product and sharp edges. I haven't used them as yet; seems such a shame to mark them.
Ken
-
7th Jan 2018, 12:11 PM #8
Do you need to machine it hard, can it be heated to remove hardness, machined and then rehardened.
I take larger items to a local spring maker and when they get a chance it goes in with a batch of truck springs .
Just grind to size or to clean up when it comes back.
Saves heaps on cutters.
Michael
Similar Threads
-
Small mill vices, these any good?
By Com_VC in forum METALWORK GENERALReplies: 9Last Post: 12th Apr 2017, 09:37 AM -
NSW - Newcastle - Face mill - carbide- No 3morse
By bollie7 in forum METALWORK - Machinery, Equipment, MARKETReplies: 0Last Post: 25th Feb 2017, 05:03 PM -
source of good aussie hss endmills
By the fabricator in forum METALWORK GENERALReplies: 8Last Post: 8th Oct 2013, 08:53 PM -
Good source of metal walling / roofing in Perth?
By antonylord in forum METALWORK GENERALReplies: 2Last Post: 1st Oct 2008, 05:17 PM -
Printer Maintenance Kits good source of aluminium bar stock
By joez in forum METALWORK GENERALReplies: 4Last Post: 19th May 2008, 05:03 PM