    Good Evening,

    New to the forum and eager to jump in the conversation with a new question. I recently came across a treatment done on a corrugated metal panel and would love to replicate it somehow. Does anyone know how to achieve the iridescent, metal finish in the attached image?

    Thanks in advance!

    iridescent metal panel.jpg

  2. #2
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Hi and welcome to the Metalwork Forums,
    I have seen the pattination on other metal items but not on corrugated sheets. It is possibly the latest 'in' thing stateside but I can't say it has hit Aussie shores just as yet.

    Its an effect I have seen in handmade knife handles and in jewellery applications. Check back later as some of the blokes may be still on Xmas vacation.

    This might help in the mean time.
    https://www.ganoksin.com/article/iri...patina-recipe/

    Grahame

  3. #3
    Join Date
    Jan 2012
    Location
    Melbourne
    Posts
    149

    Default

    I see an occasional car like these:
    https://www.google.com.au/search?q=i...JJwbmZVxyjVhQM

    Not nearly as subtle as the corrugated sheets.

  4. #4
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,657

    Default

    There are various methods, using heat consentrated more in one section and less in another, dipping in various chemicals, in the case of the photo it looks to me as it has been painted with a translucent paint and most likely clear coated

  5. #5
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Looks similar to the colour of passivated zinc coated screws.

    This guy gets a similar effect on carburettors: https://www.youtube.com/watch?v=Nmn94B5UUuU
    Fast forward to the end if you just want to see the result.
    Chris

  6. #6
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    I am sure jack620 is correct as you can see some of the iridescent colour on the corners of the carby.

    In my opinion, I don't think a do it at home operation is really viable, given the size of the sheets.

    This is a process that requires an industrial scale operation. I don't believe the electrolyte chemical and means of electroplating could be simply upscaled successfully from the home process. The sheer volume of electroyte and power the consumption I suspect would be very,very expensive.

    As the surface area gets larger so do the costs. In addition, the OH&S requirements may be substantial as well.

    I was a part of the hard chrome plating industry, so I do have some knowledge of the process parallels to draw upon.

    Grahame

  7. #7
    Join Date
    Nov 2008
    Location
    North Brisbane. Qld. Australia
    Age
    70
    Posts
    1,513

    Default

    Looks like a painted finish to me.
    Nev.

  8. #8
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    I agree. I'd be taking that picture down to an automotive spray place and asking what they can do like that. I remember talking to a spray painter once about cars that seem to change colour depending on the viewing angle and he described the process used - nothing particularly difficult. I suspect that is shaped glass beads or similar added to a clear coat and sprayed over the top of some corrugated iron sheet (as that is normally zinc plated, any chemical process would first have to strip the zinc = expensive)

    Michael

  9. #9
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,218

    Default

    It looks like some electroplated method and it also looks god awful.

    Corrugated iron is bad enough in a house setting, but iridescent. What were they thinking.
    Gold, the colour of choice for the discerning person.

  10. #10
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    I'm sticking with colour passivated zinc coating like this piece of artwork is made from.
    Attached Images Attached Images
    Chris

  11. #11
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Quote Originally Posted by Michael G View Post
    I remember talking to a spray painter once about cars that seem to change colour depending on the viewing angle and he described the process used - nothing particularly difficult.
    Although I believe the paint is horribly expensive. I recall my auto paint guy told me years ago it was about $800/L. May have come down in price since then.
    Chris

  12. #12
    Join Date
    Jan 2018
    Location
    Santa Monica
    Age
    39
    Posts
    2

    Default

    Appreciate all the feedback on this thread-- sounds like there are a lot of ways to go about it! Jack620 I think you've nailed it with the image of the artwork... any chance you know where that image is from or who the artist is?

  13. #13
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

  14. #14
    Join Date
    Oct 2007
    Location
    Sydney
    Posts
    3,112

    Default

    Quote Originally Posted by .RC. View Post
    It looks like some electroplated method and it also looks god awful.

    Corrugated iron is bad enough in a house setting, but iridescent. What were they thinking.
    You wouldn't like to live in a Saturday Night Fever hay shed?

  15. #15
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Those "designer" kitchens with the narrow ribbed corrugated sheet doors and drawers don't seem so bad now, do they?

Page 1 of 2 12 LastLast

Similar Threads

  1. What finish is that?
    By neksmerj in forum METALWORK GENERAL
    Replies: 1
    Last Post: 24th May 2015, 09:18 PM
  2. Threads on finishing, finish, good finish
    By steamingbill in forum METALWORK GENERAL
    Replies: 17
    Last Post: 20th Jan 2014, 06:53 PM
  3. I want a clear protective finish on shiny metal
    By woodhog in forum METALWORK GENERAL
    Replies: 3
    Last Post: 23rd May 2007, 06:47 PM
  4. Pakerizing metal finish
    By Grahame Collins in forum METALWORK GENERAL
    Replies: 6
    Last Post: 9th Apr 2007, 12:25 PM
  5. Finish on steel?
    By Schtoo in forum METALWORK GENERAL
    Replies: 7
    Last Post: 23rd Jun 2005, 10:33 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •