    Where is a good easily contacted source of 7" x 1/2" x 1.250" grinding wheels in Australia?.

    Blackwoods only stock a 60 grit alum oxide wheel. They did order me in a 3SG (part ceramic) wheel; but it is out of balance and my adapters do not have the balancing weights attached. Also the Norton range appears very limited since St Gobain took over.

    Thomas Warburton have the Kinik range, but as they closed their local branch I would have to drive to the northern Melb suburbs to order the wheels then drive back to pick them up when they are stocked from head office. The other option is to drive to the south side of Dandenong which currently too far for a round trip for me. They don't appear to do mail order.

    Forget Amazon; Amazon Australia is a pathetic joke and Amazon US are supplied by Travers Tool Co and "do not ship to Australia". There is nothing on the TTC web site about international postage anymore. Besides the days of reasonable postage costs from the US are long gone.

    Ken

  2. #2
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    Abrasiflex MELBOURNE
    Address: 82 Logis Boulevard,
    Dandenong South, Victoria, 3175
    Telephone: 03 9565 5100
    Facsimile: 03 9565 5199
    Email: [email protected]

    Kryn
    To grow old is mandatory, growing up is optional.

  3. #3
    Join Date
    Sep 2008
    Location
    texas, queensland
    Posts
    248

    Default

    trying to remember where i bought the stones for my drill sharpening machine but its locked away in the dark corner in my head .
    however it may of been "the sandpaper man " not sure though"

    johno
    'If the enemy is in range, so are you.'

  4. #4
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,726

    Default

    hi

    T Warburton should post the wheels to you, just ring them and order what you need , they are usually helpful.

  5. #5
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,657

    Default

    Any abrasive supplier should be able to source such wheels, you are specifying "tool room wheels"

  6. #6
    Join Date
    Jun 2004
    Location
    Kyabram. Vic
    Posts
    632

    Default

    China,
    180mm tool room wheels for a J&S surface grinder.

    Locally I am lucky if I have a choice of one which is usually not what of the specs I want.
    I have been through this before with the local tool supply for abrasive wheels for my tool & cutter grinder. Ordered about 12 wheels of stated specs. Only about 3 were as specified and the rest were "that's what Norton had". Took them in desperation but only a few have been suitable. Put one alum oxide cup wheel near a piece of HSS and it blues. Too hard, too fine.

    I don't want to be caught with a heap of surface grinding wheels not fit for purpose. Shame there is not one wheel that does it all; soft steel,hard steel,cast, non ferrous. Some of the suppliers to industry seem to want to deal in box quantities, not single units.

    Morrisman,
    That;s where it was handy when they had the Shepparton branch open. I could go in,select what I wanted. They would check stock and they would order it in and pick it up a week later. I will have to try by phone and see how I go.

    Abrasiflex only has one correct sized wheel 46 and 60 grit.

    Ken

  7. #7
    Join Date
    Oct 2007
    Location
    Sydney
    Posts
    3,112

    Default

    How much are you paying for the 180 mm wheels?

  8. #8
    Join Date
    Jun 2004
    Location
    Kyabram. Vic
    Posts
    632

    Default

    Pete,
    3sg was around $95-100 and white aluminium oxide sound $30 from memory. From Blackwoods.

    Ken

  9. #9
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,218

    Default

    The norton alum oxide I bought a few years ago were half that.
    Gold, the colour of choice for the discerning person.

  10. #10
    Join Date
    Jun 2004
    Location
    Kyabram. Vic
    Posts
    632

    Default

    RC

    Thanks for the kick in the shins. I just get back into the workshop and you tell me this.

    Ken

  11. #11
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,657

    Default

    Fair enough I get m wheels locally have been using the same company for twenty years, never seem to have any problems

  12. #12
    Join Date
    Oct 2007
    Location
    Sydney
    Posts
    3,112

    Default

    Quote Originally Posted by Toggy View Post
    RC

    Thanks for the kick in the shins. I just get back into the workshop and you tell me this.

    Ken
    I don't expect you're buying them by the thousand, 30 bucks a wheel from Blackwoods seems not unreasonable.

  13. #13
    Join Date
    Jun 2004
    Location
    Kyabram. Vic
    Posts
    632

    Default

    Pete,
    That is the choice of one that I have locally. No quibble about the price. Not quite right for intended use. They only stock a middle of the road wheel hopefully trying to cover everything. I have already found on the T&CG that fine, dense wheels just load up and burn the work. Coarser more open wheels cut like the wind with no burning of the work. It does passable work on hard steel but for fine finish could be about 2 grades softer. Probably needs to be coarser grit and harder; and more open structure for soft steel.

    Ken

  14. #14
    Join Date
    Jun 2008
    Location
    Victoria, Australia
    Age
    74
    Posts
    5,080

    Default

    Quote Originally Posted by Toggy View Post
    Where is a good easily contacted source of 7" x 1/2" x 1.250" grinding wheels in Australia?.
    Forget Amazon; Amazon Australia is a pathetic joke and Amazon US are supplied by Travers Tool Co and "do not ship to Australia". There is nothing on the TTC web site about international postage anymore. Besides the days of reasonable postage costs from the US are long gone.

    Ken
    Hi Ken, I buy wheels from Travers, and haven't had any problems with shipping. Maybe it's an Amazon restriction?

    https://www.travers.com/surface-grin...eels/c/297966/

    7 x 1/2 x 1.250 ceramic are about $US40

    Ray

  15. #15
    Join Date
    Jun 2004
    Location
    Kyabram. Vic
    Posts
    632

    Default

    Hello Raymond.

    Thanks for that; you had told me that some time ago; but life or almost the end of it got in the way. If I remember correctly in those days Travers had particulars on their web site for international postage. Their amazon and epay sales ads used to cater for international postage. No mention that I can find on the web site now and the other two sites are postage to the US only.
    I have had a play with the Norton 3SG again. Redressed with a new single point diamond dresser that I had. Went to an aggressive stepover (maximum on the machine and just under half wheel width) as well as a 0.002" depth of cut. I didn't think machine had enough power for the recommended 0.005" depth of cut. Too chicken as well. The wheel dress looked good and the finish on D2 was good; but with striation which I put down to balance problems. The wheel surface was still clean, open with no loading.

    The wheel dressing was quite savage on the diamond point which may give some credence to Norton's claims of requiring special diamonds for ceramic wheels.

    If Taiwan Tools would get their act together with their website without it being offline most times I try to order a new balancing wheel adapter; I can get a replacement. If not; I will forgo the other bits I was going to order and order the adapter from the UK.

    Ken

Page 1 of 2 12 LastLast

Similar Threads

  1. Tipped tool grinder wheels
    By Jon_77 in forum METALWORK GENERAL
    Replies: 18
    Last Post: 23rd Jul 2017, 09:39 PM
  2. WTB - Surface Grinder Wheels
    By electrosteam in forum WANTED TO BUY
    Replies: 4
    Last Post: 24th Oct 2016, 05:53 PM
  3. Replies: 31
    Last Post: 15th Aug 2013, 09:58 AM
  4. clean up bench grinder wheels
    By old_picker in forum METALWORK GENERAL
    Replies: 45
    Last Post: 7th Oct 2012, 12:43 PM
  5. Adapting cup wheels to a bench grinder
    By Bryan in forum METALWORK GENERAL
    Replies: 28
    Last Post: 25th Dec 2011, 06:22 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •