Where is a good easily contacted source of 7" x 1/2" x 1.250" grinding wheels in Australia?.
Blackwoods only stock a 60 grit alum oxide wheel. They did order me in a 3SG (part ceramic) wheel; but it is out of balance and my adapters do not have the balancing weights attached. Also the Norton range appears very limited since St Gobain took over.
Thomas Warburton have the Kinik range, but as they closed their local branch I would have to drive to the northern Melb suburbs to order the wheels then drive back to pick them up when they are stocked from head office. The other option is to drive to the south side of Dandenong which currently too far for a round trip for me. They don't appear to do mail order.
Forget Amazon; Amazon Australia is a pathetic joke and Amazon US are supplied by Travers Tool Co and "do not ship to Australia". There is nothing on the TTC web site about international postage anymore. Besides the days of reasonable postage costs from the US are long gone.
Ken
-
2nd Dec 2017, 07:16 PM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Abrasiflex MELBOURNE
Address: 82 Logis Boulevard,
Dandenong South, Victoria, 3175Telephone: 03 9565 5100 Facsimile: 03 9565 5199 Email: [email protected]
KrynTo grow old is mandatory, growing up is optional.
-
2nd Dec 2017, 08:16 PM #3Senior Member
- Join Date
- Sep 2008
- Location
- texas, queensland
- Posts
- 248
trying to remember where i bought the stones for my drill sharpening machine but its locked away in the dark corner in my head .
however it may of been "the sandpaper man " not sure though"
johno'If the enemy is in range, so are you.'
-
2nd Dec 2017, 09:01 PM #4
hi
T Warburton should post the wheels to you, just ring them and order what you need , they are usually helpful.
-
2nd Dec 2017, 11:07 PM #5China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Any abrasive supplier should be able to source such wheels, you are specifying "tool room wheels"
-
3rd Dec 2017, 09:27 AM #6Golden Member
- Join Date
- Jun 2004
- Location
- Kyabram. Vic
- Posts
- 632
China,
180mm tool room wheels for a J&S surface grinder.
Locally I am lucky if I have a choice of one which is usually not what of the specs I want.
I have been through this before with the local tool supply for abrasive wheels for my tool & cutter grinder. Ordered about 12 wheels of stated specs. Only about 3 were as specified and the rest were "that's what Norton had". Took them in desperation but only a few have been suitable. Put one alum oxide cup wheel near a piece of HSS and it blues. Too hard, too fine.
I don't want to be caught with a heap of surface grinding wheels not fit for purpose. Shame there is not one wheel that does it all; soft steel,hard steel,cast, non ferrous. Some of the suppliers to industry seem to want to deal in box quantities, not single units.
Morrisman,
That;s where it was handy when they had the Shepparton branch open. I could go in,select what I wanted. They would check stock and they would order it in and pick it up a week later. I will have to try by phone and see how I go.
Abrasiflex only has one correct sized wheel 46 and 60 grit.
Ken
-
3rd Dec 2017, 09:40 AM #7Most Valued Member
- Join Date
- Oct 2007
- Location
- Sydney
- Posts
- 3,112
How much are you paying for the 180 mm wheels?
-
3rd Dec 2017, 10:25 AM #8Golden Member
- Join Date
- Jun 2004
- Location
- Kyabram. Vic
- Posts
- 632
Pete,
3sg was around $95-100 and white aluminium oxide sound $30 from memory. From Blackwoods.
Ken
-
3rd Dec 2017, 04:22 PM #9Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
The norton alum oxide I bought a few years ago were half that.
Gold, the colour of choice for the discerning person.
-
3rd Dec 2017, 05:29 PM #10Golden Member
- Join Date
- Jun 2004
- Location
- Kyabram. Vic
- Posts
- 632
RC
Thanks for the kick in the shins. I just get back into the workshop and you tell me this.
Ken
-
3rd Dec 2017, 06:00 PM #11China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
Fair enough I get m wheels locally have been using the same company for twenty years, never seem to have any problems
-
3rd Dec 2017, 08:44 PM #12Most Valued Member
- Join Date
- Oct 2007
- Location
- Sydney
- Posts
- 3,112
-
4th Dec 2017, 09:08 AM #13Golden Member
- Join Date
- Jun 2004
- Location
- Kyabram. Vic
- Posts
- 632
Pete,
That is the choice of one that I have locally. No quibble about the price. Not quite right for intended use. They only stock a middle of the road wheel hopefully trying to cover everything. I have already found on the T&CG that fine, dense wheels just load up and burn the work. Coarser more open wheels cut like the wind with no burning of the work. It does passable work on hard steel but for fine finish could be about 2 grades softer. Probably needs to be coarser grit and harder; and more open structure for soft steel.
Ken
-
6th Dec 2017, 09:50 PM #14
Hi Ken, I buy wheels from Travers, and haven't had any problems with shipping. Maybe it's an Amazon restriction?
https://www.travers.com/surface-grin...eels/c/297966/
7 x 1/2 x 1.250 ceramic are about $US40
Ray
-
7th Dec 2017, 07:11 PM #15Golden Member
- Join Date
- Jun 2004
- Location
- Kyabram. Vic
- Posts
- 632
Hello Raymond.
Thanks for that; you had told me that some time ago; but life or almost the end of it got in the way. If I remember correctly in those days Travers had particulars on their web site for international postage. Their amazon and epay sales ads used to cater for international postage. No mention that I can find on the web site now and the other two sites are postage to the US only.
I have had a play with the Norton 3SG again. Redressed with a new single point diamond dresser that I had. Went to an aggressive stepover (maximum on the machine and just under half wheel width) as well as a 0.002" depth of cut. I didn't think machine had enough power for the recommended 0.005" depth of cut. Too chicken as well. The wheel dress looked good and the finish on D2 was good; but with striation which I put down to balance problems. The wheel surface was still clean, open with no loading.
The wheel dressing was quite savage on the diamond point which may give some credence to Norton's claims of requiring special diamonds for ceramic wheels.
If Taiwan Tools would get their act together with their website without it being offline most times I try to order a new balancing wheel adapter; I can get a replacement. If not; I will forgo the other bits I was going to order and order the adapter from the UK.
Ken
Similar Threads
-
Tipped tool grinder wheels
By Jon_77 in forum METALWORK GENERALReplies: 18Last Post: 23rd Jul 2017, 09:39 PM -
WTB - Surface Grinder Wheels
By electrosteam in forum WANTED TO BUYReplies: 4Last Post: 24th Oct 2016, 05:53 PM -
Where to get decent quality wire buff wheels for 8" bench grinder in Adelaide
By nearnexus in forum METALWORK GENERALReplies: 31Last Post: 15th Aug 2013, 09:58 AM -
clean up bench grinder wheels
By old_picker in forum METALWORK GENERALReplies: 45Last Post: 7th Oct 2012, 12:43 PM -
Adapting cup wheels to a bench grinder
By Bryan in forum METALWORK GENERALReplies: 28Last Post: 25th Dec 2011, 06:22 PM