Hi guys, got just of a bit of an academic question for the gurus here. I've got a metre length of 50 by 50 by 3 rhs (supported at each end and not restrained) that is to have a centre point load of 1000kgs. I need to know the deflection.
I remember doing a bit of this 30 years ago, but I'm out of touch now. Something about second moment of area
and bending moments I think. Any hellp welcome.
Eric
-
19th Nov 2017, 04:07 PM #2Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
God j remember doing those calcs using eulers questions..
Be buggered if i could do it now! Sorry.
Simon
Sent from my SM-G900I using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
19th Nov 2017, 04:30 PM #3Senior Member
- Join Date
- Dec 2007
- Location
- Melbourne
- Posts
- 103
About 76mm according to this site https://www.easycalculation.com/engi...ular-beams.php
-
19th Nov 2017, 05:15 PM #4Senior Member
- Join Date
- Dec 2012
- Location
- emerald
- Posts
- 161
-
19th Nov 2017, 07:28 PM #5Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
-
19th Nov 2017, 07:56 PM #6Senior Member
- Join Date
- Dec 2012
- Location
- emerald
- Posts
- 161
That calculator doesn't seem to give much info as far as the beam details go. I think it must be referring to a cantilevered beam , ie supported at one end and the load applied to the other. If this was the case I can well believe that deflection with 1000kgs at one end of a metre length.
-
19th Nov 2017, 08:03 PM #7Senior Member
- Join Date
- Dec 2012
- Location
- emerald
- Posts
- 161
Also this calculator should include the point of exceeding the modulus of elasticity. Deflection past this point is meaningless.
-
19th Nov 2017, 08:33 PM #8Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
The diagram under the calculator indicates the beam spans two supports. It also implies the load is evenly distributed along the beam.
Chris
-
19th Nov 2017, 09:27 PM #9Senior Member
- Join Date
- Dec 2012
- Location
- emerald
- Posts
- 161
-
20th Nov 2017, 12:34 AM #10Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,942
Thanks for the Link, grunto, hope you don't mind, I've put it at the bottom of the forums in the Conversions and Calculations section, hopefully for all members to find easily.
I know I'll be using it a fair bit
Gesalt, if your wanting to suspend the 1,000 kg off the bar, it would need to be 100 X 50 X 8 to get a deflection of 6.34 mm, going by the calculator grunto supplied.
KrynTo grow old is mandatory, growing up is optional.
-
20th Nov 2017, 01:08 PM #11Senior Member
- Join Date
- Dec 2012
- Location
- emerald
- Posts
- 161
Thanks Kryn, but there's something wrong in those calculations. I did some practical stuff this morning and suspended the load on the rhs beam (see pics) and got a deflection of around 5mm. This made more sense to me. In fact, this calculator confirms it:
Beam deflection and stress calculator
I can't really understand the example in the first calculator of a beam that is 20 inches long and 30 by 30 inches high and wide with 10 inch wall thickness. It's probably just me, but I don't get it.
Anyway it looks like I'm OK to go with the 50 by 50 .
I have to get the thing inside the house and stand it up on its footing (once it's sand blasted and painted).
Eric
-
21st Nov 2017, 05:47 AM #12Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
I have new found respect for RHS!
Chris
-
21st Nov 2017, 07:07 AM #13Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Nice. Good to see it all went OK.
What is it BTW? Looks like something from a refinery, like a cracking tower!
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
21st Nov 2017, 07:11 PM #14Senior Member
- Join Date
- Dec 2012
- Location
- emerald
- Posts
- 161
-
21st Nov 2017, 09:11 PM #15Senior Member
- Join Date
- Jun 2012
- Location
- melbourne
- Posts
- 341
I tried solid works which has a very simple wizard for simple people. it only works on single parts but you can only add simple fixtures and forces. Because your beam is not fixed either end, i drew it with the vertical arms, so there would be no force holding the beam back from bending in. SW has a complex calculator too, but by doing tricks like this I've never had to learn how to use it.
Three pictures, one shows stress, one shows displacement (~6mm) and one shows factor of safety. The red on the blue beam, is where the factor of safety is below 1.
I used a force of 10,000N and a material of AISI 1010 steel, not sure if thats right for material. For a point source, I used the forced displaced over a 10mm wide strip across the middle.
I can't even remember if i knew how to work these things out or not. You'll have to guess if i got it wrong or not but I've trusted a lot of weight on this before but I leave a FOS of 4 at least, 8 if i can afford it. The model is a pure square with 5mm outer radius but no account for the welded seam.
Similar Threads
-
Square Hollow Section Strength/Deflection charts in Metric?
By joez in forum METALWORK GENERALReplies: 10Last Post: 17th Aug 2017, 07:33 AM -
Making a Steel Beam Flat
By grunto in forum METALWORK GENERALReplies: 15Last Post: 26th Jun 2017, 09:31 PM -
Steel grate rhs deflection
By oohsam in forum METALWORK GENERALReplies: 17Last Post: 17th Jun 2016, 10:19 AM -
Building a Aluminium I Beam Trailer
By gazza2009au in forum TRAILERS & OTHER FABRICATED STUFFReplies: 58Last Post: 30th Mar 2015, 11:45 PM -
Cornish beam engine
By neksmerj in forum METALWORK GENERALReplies: 5Last Post: 22nd Aug 2013, 01:05 PM