Alternative to grinding on side of wheel ?
Would you ever use these as an alternative to grinding on the flat side of the wheel ? (Which of course we never do anyway.) Am guessing some sort of solid backing plate would be needed.
Grit 80 Diamond coated 6" inch Flat Lap wheel Lapidary grinding polishing disc | eBay
During some googling this morning I became quite confused regarding what use experienced metalworkers might have for these diamond wheels.
Have tried a few times now to get local Bunnings to "special order" me a white Norton alox cup wheel but they seem to have a lot of difficulty, and after waiting a few weeks offer me a standard grey circular wheel.
Bill
-
18th Oct 2017, 02:42 PM #2China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
I have them for use in cutting and polishing gem stones and yes I have cheated and used them for carbide and HSS wet of course and they work quite well as for alox wheels etc go to a abrasives supplier it is not really one of the areas that Bunnings exel
-
18th Oct 2017, 03:20 PM #3Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Bill, I've had one of those THK 6" diamond wheels on the side of my CBN wheel since 2014.
They do flex so it's supported backed by a 12mm thick steel disc that is is about 75mm in diameter.
Works great.
TP1.jpg
We bought a set of about a dozen different grits of these diamond lapidary wheels for SWMBO's jewellery hobby and she has used one for a few hours.
-
18th Oct 2017, 06:51 PM #4
thomas
Bill this business had a shop in Dandenong South . They used to have a large range of grinding wheels Thomas Warburton - Abrasives. They will post stuff to you . Not sure if the shop is still there in Dand. Sth anymore it was along the Sth Gippsland Hwy.
Similar Threads
-
Grinding wheel
By sossity in forum METALWORK GENERALReplies: 38Last Post: 14th Feb 2017, 06:04 PM -
Grinding Wheel
By Oldneweng in forum METALWORK GENERALReplies: 18Last Post: 15th Jan 2017, 06:07 PM -
Grinding wheel advice
By caskwarrior in forum METALWORK GENERALReplies: 1Last Post: 18th Dec 2016, 08:53 PM -
Which Grinding Wheel For Grinding Tungsten Electrodes
By Metal Head in forum WELDINGReplies: 14Last Post: 8th Aug 2009, 02:23 PM -
Lap grinding wheel
By ROB NZ in forum METALWORK GENERALReplies: 6Last Post: 20th Jan 2008, 06:42 AM