I can’t do a bad weld if I try.
As the title says...I can’t do a bad weld if I try....not sure I can do a good one either, for that matter.
I saw these amazing sculptures while I was away and I thought I could try it as a technique in my work. Bird welds happen when I don’t want them so I should be able to do this......well not when I try.
I have a small mig and old arc welder both 240v home size units.
Any suggestions?…..Live a Quiet Life & Work with your Hands
-
17th Oct 2017, 09:51 AM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Not sure how that would be done. Metal spray perhaps?
Michael
-
17th Oct 2017, 10:28 AM #3Banned
- Join Date
- Feb 2015
- Location
- Oz
- Age
- 73
- Posts
- 459
When in the industry we did a lot of peening seen on top of the leaves, done with a ball pein and anvil. Having said that, under magnification the peening is ver uniform so possibly done with a machine, a jig or a very accurate hammer man The underside just looks like spots of weld. That wouldn't take long, would it?
Brilliantly done though.
-
17th Oct 2017, 03:04 PM #4
Here’s where I went with my attempt today.
I used mug with no gas. I think it would look better with thinner if wire.
I like the concept but not happy with the results yet. While it was hot I melted in some copper accents.
I had to make a dishing stump before I started.…..Live a Quiet Life & Work with your Hands
-
17th Oct 2017, 05:32 PM #5Banned
- Join Date
- Feb 2015
- Location
- Oz
- Age
- 73
- Posts
- 459
I'd use a stick on low amps.
-
18th Oct 2017, 01:18 AM #6Golden Member
- Join Date
- Jul 2011
- Location
- Adelaide
- Posts
- 837
It could be 3d printed with laser sintering.
-
18th Oct 2017, 08:13 PM #7I break stuff...
- Join Date
- Aug 2010
- Location
- Toorloo Arm, VIC
- Age
- 39
- Posts
- 1,300
If I was trying to recreate the effect in the first picture, I'd probably try a mig with voltage set way too low, and wire feed cranked up? Should get somewhere near the result - maybe...
-
18th Oct 2017, 10:29 PM #8
A lovely squid jig for a bit of night fishing
Seriously,that beading effect occurs in the lower end of the short arc range of mig. The setting (??) can be tweaked to get that blob ball effect. It requires a trigger pull, then a quick release.yep! no gas either.
Grahame
-
19th Oct 2017, 07:10 AM #9Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,227
-
19th Oct 2017, 09:57 AM #10Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
It could have been done by that hardfacing method of putting grit tungsten carbide in the metal. Although I imagine the cost would mean it was not done that way.
Gold, the colour of choice for the discerning person.
Similar Threads
-
Weld Art?
By newbyangler in forum WELDINGReplies: 20Last Post: 5th Jun 2016, 09:01 AM -
Can you over weld ali?
By constablechris in forum WELDINGReplies: 18Last Post: 5th Feb 2012, 06:34 PM -
weld sequence
By pjt in forum WELDINGReplies: 5Last Post: 27th Sep 2009, 09:59 PM -
Bubble at end of TIG weld
By Pete F in forum WELDINGReplies: 7Last Post: 2nd Sep 2009, 07:46 PM -
teach me to weld
By kwappa in forum WELDINGReplies: 19Last Post: 25th Jun 2009, 01:26 AM