Results 1 to 9 of 9
  1. #1
    Join Date
    Jul 1999
    Location
    Glen Iris, Vic, Australia
    Posts
    42

    Default Suggestions for rounding over sharp edges on engineers square and combination squares

    Suggestions rounding over sharp edges on engineers square and combination squares?

    I've just purchased reasonably in-expensive engineers square and combination squares.

    All have sharp edges.

    Any suggestions on how to make them not so sharp?
    Should I leave them?
    Can I dull them by microns?

    Thanks in advance.
    Thanks,
    Barry G. Sumpter
    Proud Tritoneer
    ( see my other 40 posts under BarryGSumpter )

    May Yesterdays Tears Quinch the Thirst for Tomorrows Revenge

  2. #2
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Put a strip of emery on a flat surface and gently pull the edge in question along it. All you should be doing is taking the sharp off.

    Michael

  3. #3
    Join Date
    Jun 2013
    Location
    Tasmania
    Posts
    257

    Default

    A quick brush (light pass) past a wire wheel on the grinder?

    Usually enough to break the edge.

  4. #4
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,480

    Default

    Hi Barry,

    A quick swipe with a fine stone is usually enough.
    Best Regards:
    Baron J.

  5. #5
    Join Date
    Apr 2014
    Location
    Little River
    Posts
    3

    Default

    Quote Originally Posted by BaronJ View Post
    Hi Barry,

    A quick swipe with a fine stone is usually enough.
    That was going to be my suggestion as well as that's what I have done.

  6. #6
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    I found a Scotchbrite wheel is good for this sort of things,

  7. #7
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    I know a well known boutique maker uses a 3m Scotchbrite debuting wheel on his bench grinder for just this purpose on his squares.


    Sent from my iPhone using Tapatalk
    …..Live a Quiet Life & Work with your Hands

  8. #8
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Just remember that depending on the grade, that Scotchbrite can be might aggressive.

    Michael

  9. #9
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    I would use a stone too.
    Chris

Similar Threads

  1. Pre-relieving cutting edges
    By bob ward in forum METALWORK GENERAL
    Replies: 14
    Last Post: 3rd Dec 2015, 10:56 AM
  2. Precision Engineers Square
    By Oldneweng in forum METALWORK GENERAL
    Replies: 26
    Last Post: 8th Jun 2015, 09:34 PM
  3. Black Engineers Square
    By Stustoys in forum METALWORK GENERAL
    Replies: 11
    Last Post: 22nd Feb 2014, 09:48 PM
  4. B grade Engineers square, what are the tolerances?
    By simonl in forum METALWORK GENERAL
    Replies: 4
    Last Post: 2nd Aug 2012, 10:50 PM
  5. Wanted Large Engineers Square
    By johncee1945 in forum METALWORK GENERAL
    Replies: 2
    Last Post: 19th Apr 2012, 08:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •