sparkly shiny bright finish on chess pieces ?
I'd like to have a go at some chess pieces in the future
What key words should I be googling or web pages/ books should I be reading about to learn how to get a a nice sparkly bright untarnishable finish on brass and mild steel that wont be affected by greasy fingers ?
Am assuming some sort of varnish / lacquer rather than bare metal ?
Or is this where I learn how to cut stainless steel ?
Bill
-
3rd Aug 2016, 09:20 PM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Hi Bill,
After you've made the pieces, polish them and then have them powder coated, or do them in a clear automotive finish. If you have them powder coated, drill and tap 3 or 4 mm threads in the bases for them to be wired for P/Coating.
KrynTo grow old is mandatory, growing up is optional.
-
3rd Aug 2016, 10:01 PM #3Senior Member
- Join Date
- Jan 2012
- Location
- Melbourne
- Posts
- 149
l have used Incralac, spray cans. Good results.
http://www.wattyl.net.au/nztechnical...etal/WM326.pdf
-
7th Aug 2016, 10:16 PM #4Golden Member
- Join Date
- Nov 2010
- Location
- Gippsland Victoria
- Posts
- 733
Thanks for the replies. Google revealed a similar question posted in another forum.
Responses on that forum included hairspray, shellac, 50/50 "Rustins" and acetone, Linseed oil and "thinners"
and this stuff ; Diamond Finish Clear Coat Information and Instructions
this is the Rustins ; Metal Lacquer at Rustins
Bill
-
8th Aug 2016, 09:22 PM #5China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
I have used the Rustins before with no problems
-
8th Aug 2016, 09:48 PM #6Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
One of the interesting things about stainless steel is the range of colours it goes when heated (that is, the colours of the oxides), so you could have one part of the set left natural and the other oxidised to a deep purple/ blue
colours.jpg
Provided that your design is not overly complex and your lathe/ mill has some rigidity, S/S should not be a problem (as every one tells me when I complain about S/S). The main issue that presents with S/S is that it will work harden, so decent cuts, preferably carbide if you can and try to keep the cut cold if using HSS otherwise it will blunt tools.
One of the downsides with lacquers is over time they will wear/ fail so they will need to be done again - that could be 10, 15 or more years down the track but it's not do once and forget.
Michael
-
8th Aug 2016, 10:44 PM #7Golden Member
- Join Date
- Nov 2010
- Location
- Gippsland Victoria
- Posts
- 733
Thanks Michael, didnt know that ............... or rather ........ one part of my brain just said "Of course I've seen that before ! What a good idea that would be interesting to try" ............ the other parts of brain that were controlling this particular chess set idea have been given a good kicking and told to wake up.
Will have a few test runs in the shed on various things suggested above.
Bill
-
10th Aug 2016, 10:39 PM #8New Member
- Join Date
- Aug 2016
- Location
- Lowood QLD Australia
- Posts
- 1
Hi there. I read just recently where a chap who had made his own chess men from bronze obtained a lovely shine through tumbling them in a home-made tumbler... fabricated from a vegemite jar filled with nuts. I think he said it took about 4 hours to get the level of shine he wanted. The mental image he created in my mind was a tumbler which looked similar to a concrete mixer! Hope that helps. You can obtain small motors from Jaycar Electronics... Vegemite jars from... HA!
Similar Threads
-
Threads on finishing, finish, good finish
By steamingbill in forum METALWORK GENERALReplies: 17Last Post: 20th Jan 2014, 06:53 PM -
polishing the shiny bits
By tanii51 in forum METALWORK GENERALReplies: 2Last Post: 3rd Oct 2010, 10:04 PM -
Polishing the shiny bits
By neksmerj in forum THE HERCUS AREAReplies: 11Last Post: 2nd Dec 2008, 05:05 PM -
I want a clear protective finish on shiny metal
By woodhog in forum METALWORK GENERALReplies: 3Last Post: 23rd May 2007, 06:47 PM