    Default Can anyone.Identity the Brand

    I have started restoring this tilting sine vice. The only marking on.it is a P with an arrow.under it. I Believe it's European as there is a Din number on the handle.
    Attached Images Attached Images
    BETTER TO HAVE TOOLS YOU DON'T NEED THAN TO NEED TOOLS YOU DON'T HAVE

    Andre

  2. #2
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,656

    Default

    Looks like a Palmgren

  3. #3
    Join Date
    Nov 2008
    Location
    Perth WA
    Age
    71
    Posts
    6,458

    Default

    I'm not sure China, I reckon it looks too refined to be a Palmgren. I have one of their catalogues along with a few others and I will have a look tomorrow to see if I can come up with anything.

    Bob.


    OK , I've had a look through through the catalogues and the closest but not close enough is Palmgen's 45V. The finish is far removed in reality from the catalogue illustrations.

    DSC_5930 (Large).JPG DSC_5938 (Large).JPG DSC_5937 (Large).JPG DSC_5941 (Large).jpg

    There are a few Parkinson machine vices featured in the McPherson's catalogues but not a tilter though that doesn't mean they didn't make one. Anyway, it is a good looking substantial vice. Nice find Andre.

    Bob.
    Last edited by Anorak Bob; 20th Apr 2016 at 12:34 PM. Reason: Photos added.

Similar Threads

  1. QCTP brand ?
    By morrisman in forum METALWORK GENERAL
    Replies: 16
    Last Post: 4th Sep 2015, 07:12 PM
  2. LIMIT brand
    By WesP in forum METALWORK GENERAL
    Replies: 4
    Last Post: 17th Apr 2015, 05:51 PM
  3. Carefull with this brand
    By matthew_g in forum WELDING
    Replies: 3
    Last Post: 24th Apr 2012, 11:21 PM
  4. Pipe Vice-pipe bender identity and info please
    By Log in forum METALWORK GENERAL
    Replies: 18
    Last Post: 18th Apr 2012, 01:14 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •