    Default Acid resistant brass screws

    I tried to turn some brass wood screws a copper colour by putting in a weak acid solution (to eat the zink away) in order to match a copper alloy casting. The weak acid made no progress at all so I upped the strength and left them in over night. Next morning still bright brass colour, so went over them with 000 steel wool in case they had some sort of protective coating and repeated the process --- still nothing. In desperation I took to them with Hcl acid and still nothing. The screw are very old perhaps 40 to 50 years, but I have never come across any brass before that is so acid resistant.

    Has anyone ever encounted this type of resistance? Normally you only have to show acid to brass and it turns red in fright.

    Bruce

  2. #2
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,188

    Default

    Are you sure they are brass. If they are bronze, especially Al bronze that is resistant to HCl at room temp.
    The HCl should have an effect at higher temperature or try some Nitric or sulphuric acid.

    see The Hendrix Group > Resources > Material Property Data > Copper and Copper Alloys > Copper Corrosion Resistance Data

  3. #3
    Join Date
    Mar 2013
    Location
    south coast Australia
    Posts
    26

    Default

    Thanks for the reply. I suspect you're on the right track, and I hadn't thought of that. The outer pack is missing so nothing to go by. Looking through the other packets of brass screws (all marked and of the same age) unsurprisingly they are all tarnished, but the screws in this pack are all shiny, and they wouldnt be the case if they were brass.
    Bruce

Similar Threads

  1. M8 Tee Nuts and Brass Tipped set Screws.
    By Gestalt in forum METALWORK GENERAL
    Replies: 3
    Last Post: 13th Apr 2015, 08:26 AM
  2. Strength of phosphoric acid?
    By nadroj in forum METALWORK GENERAL
    Replies: 28
    Last Post: 27th Nov 2011, 10:13 AM
  3. Where to find hydrochloric acid?
    By Pete F in forum WELDING
    Replies: 16
    Last Post: 8th Nov 2009, 04:49 PM
  4. Acid bath strength
    By JillB in forum METALWORK GENERAL
    Replies: 5
    Last Post: 12th May 2008, 11:58 AM
  5. Hydrochloric acid for Damascus?
    By ohno in forum METALWORK GENERAL
    Replies: 10
    Last Post: 10th Oct 2006, 09:49 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •