    Default Band saw Cutting a Car in Half

    Just saw this today. What's the size of this band saw ?

    http://sawblade.tv/video/curiosity-s...-subaru-car-2/

  2. #2
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,218

    Default

    Bit gimmicky to me.

    Cutting 1mm sheet steel is not much to spruik about...

    Now if they had have sectioned the engine lengthways...

    Now this is cutting http://www.theatlantic.com/technolog...-pieces/59656/
    Gold, the colour of choice for the discerning person.

  3. #3
    Join Date
    Jan 2007
    Location
    Katoomba NSW
    Posts
    209

    Default

    Quote Originally Posted by bosox View Post
    J What's the size of this band saw ?
    60 inch. And it would have been more impressive if they cut it long ways.
    Built: a Bench,a Desk,an Archery Display,

    Those were the droids I was looking for.

  4. #4
    Join Date
    Apr 2010
    Location
    Rural Victoria
    Posts
    358

    Default

    When I was a youngster I was most impressed with my brother's ashtray that he made by cutting through a piston on the axis of the gudgeon.

    Years later.... meh....

  5. #5
    Join Date
    Jun 2012
    Location
    boston
    Posts
    43

    Default

    Quote Originally Posted by .RC. View Post
    Bit gimmicky to me.

    Cutting 1mm sheet steel is not much to spruik about...

    Now if they had have sectioned the engine lengthways...

    Now this is cutting http://www.theatlantic.com/technolog...-pieces/59656/

    Wow! That's a jaw dropper. How did they sawed it in half? What kind of band saw that can do it.

  6. #6
    Join Date
    Jun 2012
    Location
    boston
    Posts
    43

    Default

    Quote Originally Posted by NCArcher View Post
    60 inch. And it would have been more impressive if they cut it long ways.

    Thanks for the info. Yea, I agree with you. I wish they'll do something more massive cutting like .rc. posted/ .

  7. #7
    Join Date
    Oct 2004
    Location
    Southern Highlands NSW
    Posts
    1,898

    Default

    I knew someone who reckoned he often cut cars up using a woodworking hand held circular saw. Possibly a little dangerous?
    Something I tried is cutting sheet steel with a circular saw, with the blade mounted backwards (not a tipped blade). This cuts by friction, and produces less of a burred edge.

    Jordan

  8. #8
    Join Date
    Nov 2013
    Location
    Brisbane
    Posts
    102

    Default

    Quote Originally Posted by nadroj View Post
    I knew someone who reckoned he often cut cars up using a woodworking hand held circular saw. Possibly a little dangerous?
    Something I tried is cutting sheet steel with a circular saw, with the blade mounted backwards (not a tipped blade). This cuts by friction, and produces less of a burred edge.

    Jordan
    I once cut up a car with a jigsaw...

  9. #9
    Join Date
    Mar 2008
    Location
    nowra
    Posts
    1,598

    Default

    Quote Originally Posted by bosox View Post
    Wow! That's a jaw dropper. How did they sawed it in half? What kind of band saw that can do it.
    Diamond Wire It was an amazing operation like all heavy salvage

    BETTER TO HAVE TOOLS YOU DON'T NEED THAN TO NEED TOOLS YOU DON'T HAVE

    Andre

  10. #10
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Not impressed at all ..6mm or thereabouts of . It is no test to the capacity of the bandsaw, at all. The harmonics transmitted from the sheet steel might be interesting though.

    If you think about it, the pitch of the saw teeth would be no where suited to the sheet thickness.Ie not a real market for sawing single thickness sheet metal on edge.

    IMHO the clip is an out and out gimmick and does little to demonstrate the capabilities and qualities of the blade.To those who use the larger size bandsaws a lot, it wouldn't provide them a good reason to switch blades

    It sounds like this company may be a new player in the market and are seeking recognition. Was it me ,deaf as a post or did the presenter offers very little in the way of information about the blade specs .its feed rate and feet per minute.

    Saw a bulldozer in half - that WILL impress me.

    EDIT OK ! Sawing a ship in pieces and underwater to boot,is impressive . It is almost like something from a James Bond movie .

    Grahame

  11. #11
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,218

    Default

    Quote Originally Posted by Gammaboy View Post
    I once cut up a car with a jigsaw...
    I once cut the top off a caravan with a chain.... It involved two trees a tractor and a strong chain... instant flat top trailer
    Gold, the colour of choice for the discerning person.

  12. #12
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Quote Originally Posted by .RC. View Post
    I once cut the top off a caravan with a chain.... It involved two trees a tractor and a strong chain... instant flat top trailer
    But was it done with Precision and did it take time ?

    I have seen farmers cut down trees with two tractors and a strong chain