    Default Steel for below ground use

    Hello

    I'm want to insulate the edge of slab of an existing building. My idea is to insulate it with rigid polystyrene or polyurethane board the board would extend from near the bottom of the weather boards to the ground level (~125mm) and below ground (~350-400mm). To stop the foam from being damaged I want to face the foam with something that will last and look reasonably attractive. The soil is highly reactive clay so it will experience extended periods where it is wet.

    I was thinking about using Corten steel ~2mm thick, bent to slide under the weather boards, across the top of the insulation and down one face into the ground protecting the insulation. However when I've read up on Corten steel it seems its protective qualities are based on wet and drying cycles (i.e. exposed to air). This wouldn't be happening for the section that is below ground. So there's probably no benefit in using this.

    I've thought of colourbond but I'm not sure how that will last. I've seen the bottom of fences look pretty ratty in no time. I've stored some "ordinary" hot rolled sheet under the house for a while and that's turned into sheets of rust. So I'm not sure how that's going to go. However I've seen steel used for retaining walls along water courses and the building is on steel screw piles. So it is used below ground. I'm wondering if there's a grade of steel that specified for below ground use?

    Christian

  2. #2
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    You may be better off with plain steel bent up and then hot dipped galvanised. The other option (or even additional option) is an epoxy paint - the sort they use on boats.

    Michael

  3. #3
    Join Date
    Nov 2008
    Location
    Perth WA
    Age
    71
    Posts
    6,459

    Default

    316 Stainless sheet. And maybe a coating below ground of bituminous epoxy. I ask around tomorrow at work Christian.

    BT

  4. #4
    Join Date
    Oct 2004
    Location
    Southern Highlands NSW
    Posts
    1,898

    Default

    I want to do that around my slab too, but only up to ground level.
    Actually, as there will be paving, up to just under the pavers.
    The slab edge is 30cm high, and I'll leave a few inches of the edge visible, so I can see if termites try to come up.
    I've painted the slab edge with bitumen.

    Jordan.

  5. #5
    Join Date
    Jun 2011
    Location
    Australia east coast
    Age
    71
    Posts
    2,713

    Default

    Galvanised or 316 stainless. 304 if you must, it'll probably be ok.

    Depends on how long you want it to last.

    PDW

  6. #6
    Join Date
    Oct 2012
    Location
    Australia
    Posts
    621

    Default

    Just to throw another option out there maybe some plastic sheet in a colour that would suit. Dotmar have some interesting stuff.
    -Josh

  7. #7
    Join Date
    Jun 2008
    Location
    Victoria, Australia
    Age
    74
    Posts
    5,080

    Default

    Hi Christian,

    Interesting problem, I agree with BT and PDW that stainless might be the best choice, if you can find someone manufacturing food handling equipment, like restaurant kitchen stuff, they might have scrap material. and offcuts, or maybe a laser cutting place?

    A few strategically placed folds could add rigidity and allow thinner sheet?

    Of course if you wanted to go a little upmarket you could copy the Guggenheim in Bilbao which used titanium sheeting to clad the entire building...

    Regards
    Ray

  8. #8
    Join Date
    Nov 2008
    Location
    Perth WA
    Age
    71
    Posts
    6,459

    Default

    How about fibre cement sheet. Corrosion free. Cheap.

    BT

    Edit. Would require a neat zed flashing tucked up behind the boards.

  9. #9
    Join Date
    Jan 2009
    Location
    Adelaide
    Posts
    16

    Default

    Christian,
    the place I work for uses lots of steel poles buried in the ground. We have tried for a lot of years to prevent the corrosion that happens at the ground line. Galvanising doesn't work (or at least the gain in time is only very small). The bits above ground and those that are deep down will be protected, but exactly where you want the protection at the surface level, not so good.

    Now, without any actual experience to back it up I would go for stainless steel or something non metallic as has been suggested.

    If you do use metal, a bitumen finish will help a lot as Jordan and Anorak Bob have indicated. A company called Denso make various tapes for corrosion protection, they might have something of use, either over your metal or direct onto your polystyrene (in place of the metal).

    Regards
    SWK

  10. #10
    Join Date
    Jun 2011
    Location
    Australia east coast
    Age
    71
    Posts
    2,713

    Default

    Quote Originally Posted by Anorak Bob View Post
    How about fibre cement sheet. Corrosion free. Cheap.
    Relatively fragile. BT, DT.

    Thinking on it a bit more, I'd go for plastic myself. Depends on how deep you need to go really. UV stabilised black plastic is pretty good stuff.

    PDW

  11. #11
    Join Date
    Jan 2011
    Location
    Far West Wimmera
    Age
    63
    Posts
    4,049

    Default

    Quote Originally Posted by swk View Post
    Christian,
    the place I work for uses lots of steel poles buried in the ground. We have tried for a lot of years to prevent the corrosion that happens at the ground line. Galvanising doesn't work (or at least the gain in time is only very small). The bits above ground and those that are deep down will be protected, but exactly where you want the protection at the surface level, not so good.

    Now, without any actual experience to back it up I would go for stainless steel or something non metallic as has been suggested.

    If you do use metal, a bitumen finish will help a lot as Jordan and Anorak Bob have indicated. A company called Denso make various tapes for corrosion protection, they might have something of use, either over your metal or direct onto your polystyrene (in place of the metal).

    Regards
    SWK
    I agree that galv will not work at ground level as I found out after a certain dog dug up my implement shed looking for rabbits and buried the ends of a lot of galv steel.

    I would also suggest a bitumen type coating.

    Dean

  12. #12
    Join Date
    Nov 2008
    Location
    Perth WA
    Age
    71
    Posts
    6,459

    Default

    Quote Originally Posted by PDW View Post
    Relatively fragile. BT, DT.

    Thinking on it a bit more, I'd go for plastic myself. Depends on how deep you need to go really. UV stabilised black plastic is pretty good stuff.

    PDW
    How about a combination of cheap FC sheet below ground with a more durable sheet metal buried a shallow (less expensive) depth, protecting the exposed above ground expanse?

    Villaboard is compressed FC sheet , supposedly impact resistant but with a soft foam backing that resistance may be tested when Christian's kids take up cricket.

    Cheap, thin Hardieflex would be up to the subterranean task if provided with secondary protection above ground.

    Over here, I'd be nervous about plastic Peter. Over in your necks of the woods, sun damage would hardly exist.

    BT

  13. #13
    Join Date
    Jun 2011
    Location
    Australia east coast
    Age
    71
    Posts
    2,713

    Default

    Quote Originally Posted by Anorak Bob View Post
    Over here, I'd be nervous about plastic Peter. Over in your necks of the woods, sun damage would hardly exist.

    BT
    It was my Sydney house where I found out the f/c won't last.... and the black plastic does.

    Strips of Villaboard might do it.

    One of the really nice things about Tasmania is, no f*****g termites. Just as well too or half the city would disappear. I used all treated timber for the bottom plates etc when I built my house.

    My big power poles are 125mm RHS galvanised and they're wrapped in Densotape at the ground level before the hole is backfilled with concrete. The ones I had to pull out for bigger ones when I upped the wires to 3 phase were all fine. Not practical for this purpose though.

    PDW

  14. #14
    Join Date
    Jun 2008
    Location
    Newport, Victoria
    Posts
    117

    Default

    Thanks for all the suggestions.

    I was thinking of adding some sort of bitumen coating to the steel to add some extra protection especially at ground level due to that's where its going to cop corrosion.

    Part of the project is vanity as i'd like to hide the exposed slab and insulation. So I don't think cement sheeting is going to do it. Plastic is probably the choice in terms of lasting in the ground but.... i'd probably prefer the look of rust. I guess for the same reason I don't like plastic tools....

    The cost of 316 is probably going to be a deal breaker but I might use a narrower section for the exposed section and use plastic behind it going underground pretty much as BT suggested.

    BTW I think cricket is the least of my worries, my kids are into backyard science I'm more worried about them blowing something up ).

    Christian

  15. #15
    Join Date
    Jan 2011
    Location
    Far West Wimmera
    Age
    63
    Posts
    4,049

    Default

    Quote Originally Posted by CGroves View Post
    Thanks for all the suggestions.

    I was thinking of adding some sort of bitumen coating to the steel to add some extra protection especially at ground level due to that's where its going to cop corrosion.

    Part of the project is vanity as i'd like to hide the exposed slab and insulation. So I don't think cement sheeting is going to do it. Plastic is probably the choice in terms of lasting in the ground but.... i'd probably prefer the look of rust. I guess for the same reason I don't like plastic tools....

    The cost of 316 is probably going to be a deal breaker but I might use a narrower section for the exposed section and use plastic behind it going underground pretty much as BT suggested.

    BTW I think cricket is the least of my worries, my kids are into backyard science I'm more worried about them blowing something up ).

    Christian
    I would imagine that the cost of SS would be very high. If you don't like the idea of plastic then that is out. I did however just think of fake plastic weatherboards. They are very nice looking. Very natural looking etc. Just joking. I have a couple that I have been saving for that perfect job. They are quite thick and very strong. The problem is they are white and plastic.

    Hardies wall planks are FC but are thick and from what I have seen quite strong. I also have a couple of them LOL. They are available in woodgrain surface and colours these days.

    Dean

Similar Threads

  1. How to ground your welder?
    By NewLou in forum WELDING
    Replies: 49
    Last Post: 12th Nov 2007, 07:41 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •