    I'm making a backstop to prevent the chance of the dividing head sliding out of the swivel base and onto the concrete floor when the head is mounted vertically on my mill. Rather than chip more of the already chipped paintwork, I want to incorporate a plastic bumper in the vertical leg of the angle. I have a 2 inch diameter short length of nylon. Easy enough to turn but it appears too soft. What ever plastic I use I'm hoping that it is rigid enough the ensure repeatability should the dividing head be removed then reinstalled. The plastic bumper would be about 7 - 8 mm in diameter by about 3mm thick with a spigot turned on the back to enable press fitting into the angle. The plastic has to be black.

    I'm thinking of some over the counter item that could be turned down. Something like a plastic tap washer but they tend to be white. I don't mind buying some plastic rod from one of the industrial suppliers over here. Just needs to be the right rod. Any suggestions?

    BT
    Attached Images Attached Images

  2. #2
    Ueee's Avatar
    Ueee is offline Blacksmith, Cabinetmaker, Machinist, Messmaker
    Join Date
    Dec 2011
    Location
    Canberra
    Age
    39
    Posts
    4,515

    Default

    Hi Bob,
    I would go with some delrin. Comes in Black or white and is nice and hard so repeatability should not be a problem. The only problem is you will have to make it a press fit, it cannot be locktighted or glued in any way.
    1915 17"x50" LeBlond heavy duty Lathe, 24" Queen city shaper, 1970's G Vernier FV.3.TO Universal Mill, 1958 Blohm HFS 6 surface grinder, 1942 Rivett 715 Lathe, 14"x40" Antrac Lathe, Startrite H225 Bandsaw, 1949 Hercus Camelback Drill press, 1947 Holbrook C10 Lathe.

  3. #3
    jatt's Avatar
    jatt is offline Always within 10 paces from nearest stubby holder
    Join Date
    Aug 2008
    Location
    Bendigo
    Age
    51
    Posts
    760

    Default

    2nd the Delrin
    Frisky wife, happy life. ​Then I woke up. Oh well it was fun while it lasted.
    From an early age my father taught me to wear welding gloves . "Its not to protect your hands son, its to put out the fire when u set yourself alight".

  4. #4
    Join Date
    Jun 2008
    Location
    Victoria, Australia
    Age
    74
    Posts
    5,080

    Default

    Hi BT,

    I'd go for a stroll through the homewares section of your local department store, it's amazing what you can find when you start looking at everyday kitchen utensils and stuff with a different eye.



    Regards
    Ray

  5. #5
    Join Date
    Mar 2011
    Location
    Dural NSW
    Age
    82
    Posts
    1,203

    Default Suitable Plastic

    Bob
    I have some offcuts in a black plastic, tough stuff thats machinable, cannot remember the name of it at the moment. (This happens as one gets older)
    I will mail you a piece in the morning.
    regards
    Bruce

  6. #6
    Join Date
    Nov 2006
    Location
    Heidelberg, Victoria
    Age
    79
    Posts
    2,074

    Default Type of plastic

    Bob, I'd go with acetal. It's easy to machine and fairly hard. Great stuff.

    Ken

  7. #7
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,542

    Default

    I think I have a small diameter piece of black acetal somewhere if you want to try it out.

    Michael

  8. #8
    Join Date
    Nov 2008
    Location
    Perth WA
    Age
    71
    Posts
    6,458

    Default

    Thanks for the suggestions Boys.

    Bruce and Michael,
    Only if it's not too much trouble.

    Bob.

  9. #9
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Yep, Delrin (acetyl) is the go. It can be glued with epoxy. Dupont recommend sanding with 280 grit to improve the bond.

  10. #10
    Join Date
    Jun 2012
    Location
    Germany, Outback of Munich
    Posts
    211

    Default

    Delrin (POM) is hard to glue, to say the least. You can flame it or better etch with phosphoric acid.
    PA would be good for a stop, but also not something you like to glue.