Thanks Thanks:  0
Likes Likes:  0
Needs Pictures Needs Pictures:  0
Picture(s) thanks Picture(s) thanks:  0
Results 1 to 7 of 7
  1. #1
    Join Date
    May 2010
    Location
    Perth
    Posts
    135

    Default source of silver solder other than BOC?

    Folks,

    I've moved house and a large amount of my shed is packed into a storage container whilst I get the house sorted out, and look at shed erection/construction.

    As a result I will need to grab some silver solder for a few small jobs coming up.

    Last time I bought Silver solder was through BOC and it was quite expensive... is there a cheaper source of silver solder in Oz?
    I'd be chasing 2-3 rods suitable for brass, copper, steel, etc - ie general construction use - not jewellry

    I now live in the Perth area, so the big green shed, coventries, and other stores are at most 2 hours drive - most around 1 hour drive.

    if you can suggest a source, and grade of silver braze I'd appreciate it.. I do have my flux available (Sil Braze? - the one from BOC in the small balck jar), but no rods.

    Many thanks,
    Des

  2. #2
    Join Date
    Jul 2011
    Location
    Melbourne Australia
    Posts
    1,376

    Default

    Des.

    Most good Industrial suppliers usually have it by the stick. 45% seems to be pretty general purpose.

    Phil.

  3. #3
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    plumbing stores Reece etc, refrigeration wholesalers, Actrol, Heatcraft would all have it

    keep away from anything less than 15% silver brown tip...this is good for copper..no flux if clean copper
    if you want to do steel to copper then 45% Blue tip..needs flux

    both will do copper to brass with flux

  4. #4
    Join Date
    Apr 2004
    Location
    Notting Hiĺl (Melb) or Echuca
    Age
    64
    Posts
    179

    Default

    One thing I found was the last time I bought some the local welding supply place sold me the non-cadmium bearing 45% silver brazing alloy. It is OK but a slightly higher melting point and not as good on bonding to steel (from my novice perspective)

    Thus I'd be asking for the old 245SBA - cadmium bearing, 45% silver --- this is of course provided the job does not involve water or food handling equipment/utensils.

    From the modelling magazines, it would seem the cadmium bearing alloys are now much less available in the UK than previously -- Reeves ran a series of advertisements saying "this is the last batch"

    Added Link: SBA - Victoria include cadmium bearing alloys and have a "contact us" page.
    Last edited by HavinaGo; 29th Aug 2012 at 06:36 PM. Reason: added link to australian supplier of cadmium bearing alloys
    cheers
    David

    ------------------------------------------------
    A society grows great when old men plant trees whose shade they’ll never sit in. (Greek proverb)

  5. #5
    Join Date
    May 2010
    Location
    Perth
    Posts
    135

    Default

    definitely need steel to steel in the first job on the "to do" list.. so that limits me to 45% then

    I'll keep hunting around the local area before heading to Perth

    Thanks for the heads up on the 15% stuff because the local plumbing place offered that, and the "big green shed" dropped the calls each time I was transferred around the store between tool shop and plumbing.

    Thanks all,
    Des

  6. #6
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    Quote Originally Posted by desbromilow View Post
    definitely need steel to steel in the first job on the "to do" list.. so that limits me to 45% then

    I'll keep hunting around the local area before heading to Perth

    Thanks for the heads up on the 15% stuff because the local plumbing place offered that, and the "big green shed" dropped the calls each time I was transferred around the store between tool shop and plumbing.

    Thanks all,
    Des
    plumbers also use 5% and sometimes 2% if they are really rough...dont use it..make sure its 15% SBA115 or equivalent..it should have a brown tip and ideally 15% stamped on it...it may cost a little more and i mean only a little so dont skimp

  7. #7
    Join Date
    Jul 2007
    Location
    Perth
    Posts
    332

    Default

    Des,
    You could try Gentronics in Welshpool, they handle a lot of welding / brazing stuff, prices can be a bit hit and miss though. Alan.

Similar Threads

  1. brazing/silver solder help
    By fxst in forum METALWORK GENERAL
    Replies: 26
    Last Post: 7th Nov 2011, 09:47 AM
  2. Silver Solder Pt 2 How to
    By Grahame Collins in forum METALWORK GENERAL
    Replies: 0
    Last Post: 11th Jan 2007, 10:51 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •