taps and dies
hi,
I was wondering if anyone had a link to what size drills to use with metric taps.
what I mean is, if for example I have an M10 bolt and I want to tap a hole for it in some mild steel, obviously I cant use a 10mm drill or there will be no steel left for the tap to cut a thread into.
on the other extreme, the largest drill bit I have that will fit into a hole threaded for an M10 bolt is 8.5mm. (Drill bit set has .5mm increments)
I have searched google and only got imperial data. surely there is a metric chart out there somewhere? the action of tapping probably reduces the diameter of the hole a bit, so I am thinking if I drilled it at 8.5 it would be too small so is it 9mm or 9.5mm?
If I go too small I risk placing too much pressure on the tap as it is in use and risk breaking it or if I go too large there wont be enough metal in the hole to tap properly and it will strip too easily.
Does anyone have access to a chart for metric threads? greatly appreciated if someone can help me.
Doug
-
10th Mar 2012, 12:34 AM #2Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,887
Just do a search for metric tapping drill chart,if thats to hard look at the tap or taps you will be using,they are marked showing diameter of the tap and the pitch of the thread,for metric threading subtract the pitch from the tap diameter and that will be the size to drill the hole.
This is far to much information allready given for something that is all to excessable on the net.
-
10th Mar 2012, 01:09 AM #3Member
- Join Date
- Jan 2012
- Location
- South Africa
- Age
- 76
- Posts
- 53
Doug,
Here you go mate Tap Drill Sizes
For your 10 mm thread the 8.5mm drill will be fine.
I'm happy to help
Ignore 'pipeclay' seems he's a misserable so & so
Dave'H
-
10th Mar 2012, 01:27 AM #4Member
- Join Date
- Jan 2012
- Location
- South Africa
- Age
- 76
- Posts
- 53
Doug,
This one is in PDF form so you can download it and print it.
http://www.boltsupply.com/catalogue_...ta/pdf/022.pdf
Dave'H
-
10th Mar 2012, 01:32 AM #5.
- Join Date
- Nov 2008
- Location
- Perth WA
- Age
- 71
- Posts
- 6,458
-
10th Mar 2012, 02:24 AM #6Dave J Guest
Hi Doug,
Metric is the easiest of them all, like Pipeclay said you subtract the pitch from the tap diameter. So say for a common metric 6 x 1mm you just minus the 1 from 6 giving you a 5mm drill needed.
For general purpose threads around the home etc this system works fine, but you can get into different fits of threads in the engineering side of things, and it's gets a bit more complicated.
Here is another chart
Tap Chart Metric Threads
Dave
-
10th Mar 2012, 06:39 AM #7Most Valued Member
- Join Date
- Sep 2011
- Location
- Ballarat
- Age
- 65
- Posts
- 3,103
-
10th Mar 2012, 08:13 AM #8Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,887
Generally its not far off the mark for me.
I am a believer in trying to help yourself first.
People shouldnt be spoon fed,if they are they will never try to help themselves.
Going by the way this thread was worded there was a knowledge shown of some form.
The search that was conducted on google must of been very short and limited.
By just using a few of the words in the posted thread results on google were achievable.
From the way the thread was written the poster has a basic knowledge of what they are attempting to do or achieve.
The thread also showed an amount of reasoning and thought,in my opinion enough to be able to search google to find the desired information.
-
10th Mar 2012, 08:38 AM #9New Member
- Join Date
- May 2010
- Location
- Not far enough away from Melbourne
- Posts
- 0
thanks for the help
Good morning everyone.
Thanks to the two Dave's for the links to the charts. That is exactly the information I was asking for.
Pipeclay, I think you might have stayed up about half an hour past your bed-time last night and got a little grumpy. But thanks for recognising that I had acquired some basic knowledge of the process, that knowledge was all thanks to google and other research I did yesterday. But try as I might I just could not find any metric charts.
Thanks again to those who helped
Doug
-
10th Mar 2012, 08:44 AM #10Most Valued Member
- Join Date
- Oct 2007
- Location
- Sydney
- Posts
- 3,112
Doug, don't worry mate, after a few years you'll learn to ignore the idiot responses on this board, it seems some people seriously need a root ... or something.
With regard the tapping drill size, the problem with metric is that the tapping drill is not normally included in standard drill sets with 0.5 mm rises such as the type you'd buy at a hardware store. Off the top of my head I think M6 and M10 are the only exceptions in sizes most people would commonly tap. However in the charts you now have you'll note the quoted tapping drill is designed to give full thread depth. Most of the time we don't need that, and the fastener will still function perfectly and be very nearly as strong if the hole is drill slightly oversized. "Proper" quality taps will come in a set of 3, and they will allow easy tapping to full thread depth, however cheap taps don't function nearly as well, and drilling the tapping hole slightly oversize will save a lot of frustration (and possibly broken taps). For example instead of drilling M8 6.75 mm (a size btw I've never seen and is a stupid figure to quote) drill it 7 mm, a size you'll have. Likewise M5 you could (carefully) drill 4.5 mm and so on. Just be careful at the small sizes or in critical applications or you'll lose too much strength. If it's important, then go to an engineering supply house and buy the correct size drill for that tap size, or if you're feeling wealthy buy a set in 0.1 mm rises ... and then guard them with your life
Hope that's of practical help.
Pete
-
10th Mar 2012, 09:01 AM #11New Member
- Join Date
- May 2010
- Location
- Not far enough away from Melbourne
- Posts
- 0
Thanks, Pete,
I have a good quality set with the three taps, taper, plug and bottom. I gave up buying cheap tools years ago. I dont even go into the tool shop at bunnings any more. I bought the tap and die set from Hare and Forbes and it was not the cheapest set they had.
With the background information you gave me, obviously gained from hands-on experience and the charts kindly provided by the two Dave's, I am sure that I will be able to complete my current project and many more to come.
As for grumpy people on forums, yes I have encountered them before and generally I believe they are a nice person having a bad day, they may have a problem in their personal life or had too much to drink or whatever. On the net as in real life I take it with a grain of salt and move on. After all next time I need some help they may be the one to provide the answer.
If you look at this thread http://www.woodworkforums.com/f36/forum-149396/ members are agreeing that you can ask the most basic question on the forum and people are all supportive and provide help. I agree that this is generally the case.
thanks again Pete
Doug
-
10th Mar 2012, 09:22 AM #12
On the subject of special size drills for metric taps, H&F sell a set of metric (coarse) taps, 3 each for sizes 3-12mm, with matching drills all in a metal case.
The other thing I have is a set of 115 drills that has all the Letter drills, all the Number drills and Imperial drills up to 1/2" in 1/64" steps.
Whilst these are not top notch quality they nonetheless come in very handy as they cover most of the sizes needed. I just drill a hole close to the final needed and then use one of these to drill to the final size.
-
10th Mar 2012, 09:24 AM #13New Member
- Join Date
- May 2010
- Location
- Not far enough away from Melbourne
- Posts
- 0
Question for Pete or anyone who knows, how does this apply to different materials being tapped? I will be tapping cast iron and mild steel in the near future and possibly other metals as the need arises.
I would imagine that cast iron being more brittle would be more difficult to tap than mild steel. Does this mean that it is more desirable to tap oversize on cast iron so there is less of it to tap, or would it be better to leave as much thread in the hole as possible, because it is more brittle, even though that will make the tapping harder and increase the risks of breaking a tap in the hole?
-
10th Mar 2012, 09:46 AM #14
Doug,
Get yourself an engineer's black book. It's the most used "tool" in my workshop. As for drill sizes for metric taps, imperial 1/64 sets cover most of the unusual sizes needed.
Ewan
-
10th Mar 2012, 10:20 AM #15Distracted Member
- Join Date
- May 2010
- Location
- Lower Lakes SA
- Age
- 58
- Posts
- 2,607
CTC tools sell individual drill bits in 0.1mm increments, quite cheaply. The quality is usually ok too. I say usually because I had one that wasn't heat treated or something because it was soft as. The others (4 or 5) have all had good geometry and performed well. Results for Cutting Tools: Drill Bits
Attached is a chart I like because it gives some guidance on thread depth.
Similar Threads
-
Storing taps dies etc.
By Tiger in forum METALWORK GENERALReplies: 16Last Post: 11th Apr 2010, 01:31 PM -
Need to borrow some taps and dies
By funkychicken in forum METALWORK GENERALReplies: 5Last Post: 8th Apr 2009, 10:04 AM -
Taps & Dies
By footz in forum METALWORK GENERALReplies: 22Last Post: 6th Oct 2008, 07:11 PM -
Hafco Taps & Dies
By fraserbluff in forum METALWORK GENERALReplies: 2Last Post: 26th Apr 2007, 12:29 AM -
Dies
By Tiger in forum METALWORK GENERALReplies: 9Last Post: 5th Dec 2005, 12:32 PM