7th Jul 2011, 04:38 PM #1Old Fart (my step daughters named me)
- Join Date
- Sep 2010
- Location
- Mallala S.A.
- Age
- 76
- Posts
- 50
Brass/Copper finish
Gents .I am not your usual turner, but I do like doing it for small pieces. As it is I have made 2 brass pens and can not keep the shine on them. That is unless I brasso them every second day. Is ther any spray on material that I can use to keep them looking nice???
-
7th Jul 2011, 05:34 PM #2Most Valued Member
- Join Date
- Jun 2007
- Location
- sydney ( st marys )
- Age
- 64
- Posts
- 4,890
Do a search for clear laquer brass/copper.
-
7th Jul 2011, 09:14 PM #3New Member
- Join Date
- Jul 2011
- Location
- Near the mountain
- Posts
- 2
I think lacquer is the easiest method.
I search via google with "protecting brass from tarnishing" and I've found that alternative methods are exist, such as gold plating and commercial brass/copper protector spray.