Hi,
I'm guessing my ways and/or gib might be worn on this 30+ year old mill.
The gib is sticking out of the back, reducing my travel by 25mm.
What to do here, cut that 25mm off, make a new gib?
Cheers
Richard "Looking for a loved 9x20 lathe" Thornton
Sydney, AU
-
17th Aug 2023, 07:11 PM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
You could although they can be tricky to make, being long and slender.
Perhaps try some thin shim behind it - even start with a layer or two of Al foil to get a feel for the thickness you need.
Michael
-
17th Aug 2023, 07:14 PM #3Senior Member
- Join Date
- Sep 2011
- Location
- Sydney
- Posts
- 232
-
17th Aug 2023, 07:20 PM #4
Abom79 did a gib repair video recently and shimmed the gib.
https://youtu.be/74MUEu0h1_g
Probably worth watching.
-
17th Aug 2023, 08:01 PM #5Diamond Member
- Join Date
- Sep 2006
- Location
- Mallacoota,VIC,Australia
- Age
- 53
- Posts
- 1,010
There is another shimming a gib video from H&W on YouTube https://youtu.be/qsKk9OajQLg which is also a good video.
All The Best steran50 Stewart
The shortest way to do many things is to do only one thing at once.
-
17th Aug 2023, 08:44 PM #6Senior Member
- Join Date
- Sep 2011
- Location
- Sydney
- Posts
- 232
Thanks, here's a photo of the front with the gib "flush" at the back, I assume it would be normal for my shimmed gib to protrude 30mm at the front?
-
19th Aug 2023, 05:19 PM #7Senior Member
- Join Date
- Sep 2011
- Location
- Sydney
- Posts
- 232
Sorry if this is a daft question but are the ways on the gib side tapered to "match" the gibs, like if the gib taper is 1:80 is that repeated (in reverse) on that side of the ways, so you get a uniform mating surface on the dovetail?
Cheers
Richard "Looking for a loved Taiwanese 9x20 lathe in Sydney" Thornton
-
19th Aug 2023, 05:31 PM #8Diamond Member
- Join Date
- Sep 2006
- Location
- Mallacoota,VIC,Australia
- Age
- 53
- Posts
- 1,010
The answer is YES the tapers would match otherwise it just wouldn't work properly. In regards to your previous question about your shimmed Gib, to me I think 30mm would be excessive unless the Gib had been originally made quite long.
All The Best steran50 Stewart
The shortest way to do many things is to do only one thing at once.
-
19th Aug 2023, 08:59 PM #9
Hi Guys,
I suspect that the gib is a little long. On my mill the gibs are about 10 mm short of the full length. When adjusted the screw head is just about flush with the casting. I have mine adjusted on the "X" so that it is very slightly tight, this removes all the end play in the table. Before adjusting "X" I could get several thou back to front rock.Best Regards:
Baron J.
Similar Threads
-
[Beginner] Are these two cuts possible on a mill?
By rthorntn in forum METALWORK GENERALReplies: 18Last Post: 9th Aug 2023, 09:14 PM -
[Beginner] Mill RPM woes
By rthorntn in forum METALWORK GENERALReplies: 14Last Post: 9th Aug 2023, 08:17 PM -
[Beginner] Can you please identify this mill component for me?
By rthorntn in forum METALWORK GENERALReplies: 7Last Post: 6th Aug 2023, 07:38 PM -
What beginner tools to get for first mill
By oohsam in forum METALWORK GENERALReplies: 29Last Post: 25th Feb 2014, 12:11 AM -
The old "trimming the mill" question
By Old Hutcho in forum METALWORK GENERALReplies: 50Last Post: 5th Feb 2014, 08:41 PM