Face Mill V End Mill
I have noted that Shell End Mills and Face mills look the same ...well at least they do to me...
What is the difference ...can any one explain?
-
30th Aug 2010, 01:57 PM #2
A face mill cuts on the end of the cutters
Attachment 146041
A shell mill cuts on the sides of the cutters.
Attachment 146042
An end mill does both but for a smaller area.
Attachment 146040
-
30th Aug 2010, 02:02 PM #3Senior Member
- Join Date
- Jul 2010
- Location
- Riverina NSW
- Posts
- 169
Usually an endmill has 4 flutes and they are used to cut keyways which are not blind and a shell mill has a lot more cutting edges and is designed to cut a fair amount off and will cut alot better when only cutting with one side than an endmill.
-
30th Aug 2010, 02:09 PM #4Senior Member
- Join Date
- Jul 2010
- Location
- Riverina NSW
- Posts
- 169
A Shell end mill is basically a facing cutting when used on a horizontal machine
-
30th Aug 2010, 02:16 PM #5Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
I thought face mills used inserts, either carbide or HSS (in the old days)
Shell end mills are smaller and are all HSS and not used today...
-
30th Aug 2010, 02:35 PM #6Senior Member
- Join Date
- Jul 2010
- Location
- Riverina NSW
- Posts
- 169
You can get shell end mills that use carbide inserts, the main difference is u use a face mill to take cuts off the face of the job and you would use a shell end mill if the majority of the cutting is on the side of the job as you ca remove more material as the cutting edge is longer.
http://img.directindustry.com/images...mill-35040.jpg
-
30th Aug 2010, 04:09 PM #7Member
- Join Date
- Aug 2009
- Location
- Lake Macquarie
- Age
- 86
- Posts
- 90
Eskimo
Try this as a reference:
Milling cutter - Wikipedia, the free encyclopedia
-
30th Aug 2010, 05:00 PM #8Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
mmm
if you ask me the shell end mill doesnt look any different than the face mill
example
Shaw Machinery Web Site
-
31st Aug 2010, 03:19 AM #9Senior Member
- Join Date
- Jul 2010
- Location
- Riverina NSW
- Posts
- 169
On that page they look the same I would call the shell end mills they have there face mills
Similar Threads
-
50mm Face Mill and 10 Mitsubishi Inserts for $CHEAP
By markjaffa in forum METALWORK GENERALReplies: 18Last Post: 11th Sep 2010, 02:23 PM -
No. 0 Mill Serial Number and Mill at Work Photos
By Anorak Bob in forum THE HERCUS AREAReplies: 1Last Post: 30th Dec 2008, 03:31 AM -
x2 mill
By beetle in forum METALWORK GENERALReplies: 0Last Post: 4th Jun 2008, 12:41 AM