Results 3,016 to 3,020 of 3020
Thread: Your latest project
-
26th Mar 2024, 05:05 PM #3016
Re broken Dowidat shifter.
Nigel I have a similar shifter with the adjusting worm missing.
I was going to weld the loose jaw to a size I need.
When I get home from Queensland I’ll measure it up and if your interested swap you as your broken jaw would suit me and you will have a complete shifter again.
H.Jimcracks for the rich and/or wealthy. (aka GKB '88)
-
29th Mar 2024, 05:35 PM #3017
Shifters or for you North Americans Crescent wrenches.
Nigel, I dug out that shifter with the missing worm and sorry it’s not a Dowidat.
I do have 10” and 12” Dowidat shifters but they’re a different series to yours?
I have a quite a few, a couple I couldn’t find, one with my fathers initials stamped on it should be in the ute.
The other possibly from somewhere in the old Russian empire has a back to front thread for adjusting the jaws.
H.Jimcracks for the rich and/or wealthy. (aka GKB '88)
-
29th Mar 2024, 05:39 PM #3018Diamond Member
- Join Date
- Aug 2019
- Location
- Revesby - Sydney Australia
- Age
- 57
- Posts
- 1,196
-
2nd Apr 2024, 07:18 PM #3019Diamond Member
- Join Date
- Aug 2019
- Location
- Revesby - Sydney Australia
- Age
- 57
- Posts
- 1,196
A sleeve
Hotrod guy comes round, wants a sleeve.
We go to his place, it is for steering column gear shift on some old Ford:
Screen Shot 2024-04-02 at 6.52.38 pm.jpg
The flange on his column is smaller than the clamp:
LK-ACA-1805_-_1_full_1.jpg
Buy some 65mm round from Edcon, bore out to 45mm:
IMG_0308.jpg IMG_0309.jpg
Make a groove, 16mm wide, 50mm dia.:
IMG_0310.jpg
bandsaw the bulk off, and face in a Hercus:
IMG_0311.jpg IMG_0312.jpg
(because it's mounted chuck jaws will actually fit in the 45mm cavity)
Then split into two shells, and deliver to the customer. A fun hour of quick machining!Nigel, from a cave FULL of unfinished projects and lost tools.
-
9th Apr 2024, 12:57 PM #3020Senior Member
- Join Date
- Jun 2020
- Location
- Freo
- Age
- 68
- Posts
- 142
I get annoyed with the toolholders not having a good place to keep them and i want to get another 5 or 6 so time to remedy the situation.
Its a bit bouncy so needs a strut from the foot but it works good
1712627485817.jpg
Similar Threads
-
latest little project