    I have a good friend who has built a CNC metal machine and he is trying to find the name of a plastic material that is used to test the pattern before using the expensive final metal. He doesn't know it's name and internet searches have not revealed the substance. However, he describes it as a pink plastic and the picture below is the material.

    CNC plastic.PNG

    Any help would be appreciated.

    Thanks

    Regards
    Paul
    Bushmiller;

    "Power tends to corrupt. Absolute power corrupts, absolutely!"

  2. #2
    Join Date
    Sep 2012
    Location
    North Yorkshire UK
    Posts
    2,166

    Default

    Hi, Try "Machinable Wax" At least that is what I think its called.
    Best Regards:
    BaronJ.

  3. #3
    Join Date
    Nov 2004
    Location
    Millmerran,QLD
    Age
    68
    Posts
    127

    Default

    Thanks BaronJ

    I think you may have nailed it straight up. I have forwarded the information.

    Regards
    Paul
    Bushmiller;

    "Power tends to corrupt. Absolute power corrupts, absolutely!"

  4. #4
    Join Date
    Oct 2011
    Location
    Adelaide
    Age
    54
    Posts
    4,915

    Default

    I think some members have made their own in the past. A mix of wax (candles?) and plastic shopping bags. A search should find something.

    Michael

  5. #5
    Join Date
    Jan 2012
    Location
    Melbourne
    Posts
    106

  6. #6
    Join Date
    Nov 2004
    Location
    Millmerran,QLD
    Age
    68
    Posts
    127

    Default

    Thanks Michael and Neil for the information.

    I have passed it on.

    Regards
    Paul
    Bushmiller;

    "Power tends to corrupt. Absolute power corrupts, absolutely!"

Similar Threads

  1. Milling Plastic? Learn How to Pick the Right Tool
    By KBs PensNmore in forum METALWORK GENERAL
    Replies: 0
    Last Post: 25th Oct 2017, 06:24 PM
  2. Large plastic chopping board at ALDI - good plastic stock
    By pippin88 in forum METALWORK GENERAL
    Replies: 1
    Last Post: 3rd Jul 2017, 10:24 PM
  3. Sacrificial Milling Plate Material
    By electrosteam in forum METALWORK GENERAL
    Replies: 7
    Last Post: 3rd Feb 2017, 08:38 PM
  4. Plastic Test Tubes for storing Taps
    By Jim Ferrous in forum METALWORK GENERAL
    Replies: 2
    Last Post: 3rd Nov 2013, 06:09 PM
  5. Which Plastic?
    By Anorak Bob in forum METALWORK GENERAL
    Replies: 9
    Last Post: 2nd Oct 2012, 02:57 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •