    Hi, I did put this over on the woodwork forums but was told I might have better luck here.. Does anyone know if any of these are any good? These are the ones here.. metal cutting technology - importers, wholesalers and manufacturers - mitsubishi carbide - quaker- vargus - azstar - drilling - milling - turning - end milling They say aussie made but just wondering if they are devent quality. They are certainly cheaper than Sutton..

    Sent from my SM-G935F using Tapatalk

  2. #2
    Join Date
    Aug 2016
    Location
    NSW
    Posts
    15

    Default

    Hi, just came across this post. Did you buy any? I used them a lot while with a previous employer & they were very good. Cheers WC57

  3. #3
    Join Date
    Apr 2018
    Location
    Toowoomba
    Posts
    6

    Default

    I sure did... So much better quality than the previous cheap chinese ones that we had. Where the cheap ones snapped after 20 minutes the exact same operation on the azstar ones were used for about 10 hrs so far and haven't looked like snapping.

    Sent from my SM-G935F using Tapatalk

  4. #4
    Join Date
    Apr 2013
    Location
    Toowoomba Qld
    Posts
    374

    Default

    Are you able to give any indication on pricing ?
    Guessing it's somewhere between Cheap Chinese & Sutton pricing but that can big a pretty big variance...

  5. #5
    Join Date
    Apr 2018
    Location
    Toowoomba
    Posts
    6

    Default

    Yeah they were $34ex for 3.0mm Ball Nose, 2 Flutes, 8mm Length of Cut
    Uncoated, Aluminium / Timber Geometry
    76mm Overall Length

    Which was still expensive but nothing on the Sutton for that kind of OAL. I think chinese ones were more like $12 each for the same but just didn't last in hardwood. Just the sound they made from the beginning was so much different.

Similar Threads

  1. AZSTAR Australian made milling cutters
    By bob ward in forum METALWORK GENERAL
    Replies: 3
    Last Post: 3rd Jul 2015, 09:51 AM
  2. What beginner tools to get for first mill
    By oohsam in forum METALWORK GENERAL
    Replies: 29
    Last Post: 25th Feb 2014, 12:11 AM
  3. Casting Tools Part 4 - Sand Casting Tools
    By RayG in forum THE FOUNDRY
    Replies: 8
    Last Post: 9th Dec 2011, 12:03 PM
  4. Arboga EM825 mill vs Hercus model 0 mill?
    By neksmerj in forum METALWORK GENERAL
    Replies: 23
    Last Post: 14th May 2011, 03:16 PM
  5. No. 0 Mill Serial Number and Mill at Work Photos
    By Anorak Bob in forum THE HERCUS AREA
    Replies: 1
    Last Post: 30th Dec 2008, 03:31 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •