Engraving Arbitrary Names
We have manufactured multiple coasters in MDF on our Mens Shed Router.
Each coaster is 86 mm square with our logo and a surround line engraved.
The plan is to have the router operating during open days and offer to engrave a visitors name on a coaster and to give it to them as a souvenir.
But, we will not have prior knowledge of the name.
So, the following methodology is proposed.
While the router is engraving a name, a second laptop will be manned at the visitor reception desk.
Input Assumptions:
- existing hardware and software to be retained; Arduino Uno, Grbl 0.9j, UGS,
- Grbl does not have options for sub-routines,
- coasters consistent size with prior engraved shed logo and surround,
- metal jig providing rigid consistent mounting of coaster.
Prior to Router Operation:
1. basic Gcode sub-program written to set up cutter at clearance height above text bottom line at centre of name (text string),
2. separate Gcode sub-programs written for all 26 letters of alphabet with each width pre-determined and noted,
3. separate sub-programs written to position cutter at text start for names of width 1 to maximum achievable,
4. basic Gcode sub-program written to move cutter to convenient safe position to allow easy coaster exchange.
During Router Operation at Second Laptop:
Visitor provides desired name to be engraved on coaster, total text width is calculated using noted letter widths,
Gcode assembled by concatenating pre-written programs:
a. basic set-up - (1) above,
b. position cutter at start of text - (3) above,
c. first letter in text - (2) above, followed by each letter in turn,
d. basic safe position - (4) above.
Gcode program transferred from second laptop to machine laptop via flash drive and stored in folder of names.
UGS loads selected program from folder of names and sends it to Grbl.
Folder of names will grow so that eventually off-line Gcode concatenation will become a minor activity.
Comments welcomed,
John.
-
11th Oct 2016, 10:37 PM #2Senior Member
- Join Date
- Oct 2015
- Location
- melbourne
- Posts
- 473
I haven't had any specific cnc routing experience, but have used a vinyl etc cutter. We drive that using inkscape and a plug-in, pretty sure there are plugins for g-code. You can then take your 'background' add in the lettering and generate your gcode. May be easier than piecing together from lots of code fragments. Of course, the gcode generated may be less than perfect...
-
12th Oct 2016, 07:14 AM #3Member
- Join Date
- Mar 2012
- Location
- adelaide
- Posts
- 91
Have you looked at "Stick Font"
NCPlot - Stick Font
its free I have used it and it works well, not on a router but A Cnc mill I assume the G code will compatible with your system
-
12th Oct 2016, 03:36 PM #4Golden Member
- Join Date
- Apr 2009
- Location
- Kingswood
- Posts
- 930
Thanks for the link to NCPlot, looks very interesting and would be much easier.
I will trial it at home tonight.
John.
-
19th Oct 2016, 04:52 PM #5Golden Member
- Join Date
- Apr 2009
- Location
- Kingswood
- Posts
- 930
Progress.
We downloaded StickFont1.1 from NCPlot and used it to engrave several names.
No real problems once we learned a few more lessons on how to operate our router.
The software seems to include simple kerning but does not allow text placed about a centre line, so it was a two-step process.
First generate a Gcode file with X=0, edit Gcode file and note last X axis cut, then calculate how far off the centre line the text string is, then re-do the Gcode generation with the X offset loaded.
Works a treat, but, the font we tried was RomanS and this does not produce proper curves for text 6 mm high with 3 digits of precision (mm).
It is all straight-line approximation.
Trying 4 digits of precision did not improve it.
For now, not a problem, but we will continue searching.
John
-
20th Oct 2016, 08:19 PM #6Member
- Join Date
- Mar 2012
- Location
- adelaide
- Posts
- 91
Glad it's going well, what is kerning ?
-
20th Oct 2016, 09:13 PM #7Senior Member
- Join Date
- Oct 2015
- Location
- melbourne
- Posts
- 473
Kerning is adjusting the spacing between letters to make it look even... Different letter pairs require different spacing.
-russ
-
23rd Oct 2016, 08:36 PM #8Senior Member
- Join Date
- Jun 2016
- Location
- Sydney
- Posts
- 283
This is built into Mach3 as a Wizard. Simple to use.
I was able to engrave numbers around a dial with it.
0690.jpg
Cheers
Roger
Similar Threads
-
Engraving Lines - A Plan
By Anorak Bob in forum METALWORK GENERALReplies: 12Last Post: 28th Aug 2012, 10:06 AM -
Tool Re-Engraving
By drsed in forum METALWORK GENERALReplies: 17Last Post: 31st May 2012, 07:42 PM -
Engraving - decent looking stuff
By Arron in forum METALWORK GENERALReplies: 6Last Post: 12th Apr 2012, 09:34 PM