Bismuth dangers
I was making bismuth crystals and thought I had enough ventilation but I was wrong. I seemed to have been exposed as now I feel very Ill. I have shivers and feel very sick. I can't concentrate and feel like I'm going crazy as well as my stomach hurts and I have a bad headache. Anybody know what I should do as it's been over 16 hours since I was melting metals and I still feel very sick.
-
11th May 2019, 10:46 AM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,559
Go see a doctor.
Michael
-
11th May 2019, 12:23 PM #3Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,188
I'd go straight to emergency.
-
11th May 2019, 10:38 PM #4Gear expert in training
- Join Date
- Aug 2008
- Location
- Melbourne
- Age
- 34
- Posts
- 1,079
Hopefully there are no significant long-term issues. Good luck
-
13th May 2019, 10:35 AM #5New Member
- Join Date
- May 2019
- Location
- 5201 s MacDill Ave Tampa fl
- Age
- 24
- Posts
- 3
I went to the emergency room and they said I had become dangerously dehydrated and low on potassium as well as there is the presence of protein in urine. They don't know if there will be further complications and recommended following up in a week. The also said bismuth is non toxic and shouldn't have caused any of the symptoms.
-
13th May 2019, 12:07 PM #6Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
Well I will give my standard answer to unknown medical conditions. Must be aids.
Gold, the colour of choice for the discerning person.
-
13th May 2019, 12:13 PM #7Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,188
Bismuth is considered less toxic than lead etc and is the active ingredient in the anti-diareahal "Pepto Bismol but unless you purchased pure Bi to start with you don't know what else is in it so you still did the right thing in going to emergency.
Protein in urine sounds like a kidney disfunction - have you been checked out for diabetes?
-
20th May 2019, 08:07 PM #8
A quick look on google I found this,
Bismuth and its salts can cause kidney damage, although the degree of such damage is usually mild. Large doses can be fatal. Industrially it is considered one of the less toxic of the heavy metals. ... May cause foul breath, metallic taste and gingivitis.
https://www.lenntech.com/periodic/elements/bi.htm
Ratty 05/2004 -05/07/2010 COOPER 01/08/1998-31/01/2012
Similar Threads
-
Dangers of breaking taps *GRAPHIC IMAGES*
By Ueee in forum METALWORK GENERALReplies: 13Last Post: 9th Nov 2015, 08:11 AM -
Dry milling aluminium dangers?
By variant22 in forum METALWORK GENERALReplies: 10Last Post: 2nd Feb 2013, 08:37 AM -
Dangers of Acetylene
By bollie7 in forum METALWORK GENERALReplies: 8Last Post: 9th Dec 2009, 10:16 AM