Thanks: 0
Likes: 0
Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 5 of 5
Thread: Anvil Question
-
10th May 2018, 05:34 PM #1Member
- Join Date
- Jul 2003
- Location
- Melbourne
- Age
- 52
- Posts
- 67
Anvil Question
Spotted this for sale near me, that casting seam looks unusual. Does that mean it cast iron? or possibly unfinished?
Description: 630 length 280 high 225 wide Brand new never used for work just been stored away
anvil.jpg
-
10th May 2018, 11:12 PM #2Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,182
I just looks an unfinished cast to me.
Some anvils have a hardface plate added to the top - depends what they are cast from.
-
14th May 2018, 04:40 PM #3
Yes that is definitely a cast anvil. You can see the parting line on the top and down below, but also the two turning lugs on the side indicate it is cast. The turning lugs also indicate it was a farriers anvil.
As to cast iron well maybe, may also be SG cast iron or cast steel. If it is common grey cast iron, it isn’t going to be much good.…..Live a Quiet Life & Work with your Hands
-
14th May 2018, 05:49 PM #4Member
- Join Date
- Jul 2003
- Location
- Melbourne
- Age
- 52
- Posts
- 67
-
14th May 2018, 05:56 PM #5
The way to test any anvil is the rebound test take a 25mm ballbearing and a 30cm ruler drop the ball bearing from the top of the ruler an see how high it bounces back up. Repeat a few times and take an average. You want at least a 70% rebound.
Cast steel should ring more than cast iron which is considered pretty dead. Cast iron will be softer and tend to dent. But don’t think they will wanting you to bash their anvil with a hammer.
If you buy it and flatten the top a spark test may give you an indication also but you have spent your money then.
Sorry I can’t be more help than that.
What do you intend to use it for?…..Live a Quiet Life & Work with your Hands
Similar Threads
-
Help with Anvil
By midlife in forum THE SMITHYReplies: 7Last Post: 26th Jul 2013, 09:54 PM -
Anvil on e Bay
By auscab in forum THE SMITHYReplies: 6Last Post: 28th Jan 2013, 10:34 PM -
SOLD: Anvil
By ranga_rod in forum METALWORK - Machinery, Equipment, MARKETReplies: 2Last Post: 25th Nov 2012, 04:15 PM -
Anvil-vise anyone seen one?