At work we have about 2000 lengths of 980mm x 75mm thin walled (1.6mm) tube that needs zinc plating. We need one hole approx 4mm diameter in one end, about 20mm in from the end, so a hook can be used to hang them. We have a drill press and I have made a simple jig to attach to drill press table. This will work by sliding the tube over the jig which consists of a piece of pipe about 75mm long just under the ID of the tube, which is attached to a piece of 75mm angle to act as a stop and to clamp or bolt to the drill table.
My question is, is there a simple idea that is better and quicker to do this job. Maybe hire some sort of punch if available?Nev.
-
26th Aug 2017, 07:55 PM #2Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
Probably belongs in the Metal Working Forum. Can a mod please move if it should?
Nev.
-
27th Aug 2017, 12:38 AM #3Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Hi Nev, It's possible to be able to punch the holes, depending on the set up of the punching machine. It would work on a similar principle to the way you're drilling them. As to hiring a machine I doubt that anyone hires them. I picked up a couple of Ficep punch and shear machines from a machinery dealer as "Parts Only", as to be able to bring them up to the OH&S standard would be horrendous, for around $400 each. By the time you add a punch and die, it could work out an expensive exercise, for a one off job. Another alternative is something similar to hand shears, but in a punch form.
Metal Guillotine Hand Lever Shear 200mm only $225
https://www.gumtree.com.au/s-ad/north-wollongong/miscellaneous-goods/metal-guillotine-hand-lever-shear-200mm-only-225/1138355637
. We also have a Bramley Hole Punch for sale... same price.
It would require some modifications to make it work for your job.
KrynTo grow old is mandatory, growing up is optional.
-
27th Aug 2017, 01:53 AM #4Tool addict
- Join Date
- May 2008
- Location
- Perth
- Posts
- 241
So long as the bit of a burr on the inside doesn't matter too much, just select a person who'd be most focused on getting it done. Sadly the majority of workers will whinge and moan about the task, far too few will relish the challenge of getting into the zone and finding a flow of getting through the work. 2,000 pieces seems like a trivial job to me, slide tube on jig drill down drill up flick tube off next tube on rinse repeat. 4mm only requires a single bit, unless you need a burr free penetration.
To me, if the burr doesn't matter, I imagine it should be a day to a day & half length job on a drill press. If no burr is necessary a punch will be a far cheaper route, if the burr doesn't matter then get someone who is least likely to let themself be distracted!
-
27th Aug 2017, 06:12 PM #5Most Valued Member
- Join Date
- Nov 2008
- Location
- North Brisbane. Qld. Australia
- Age
- 70
- Posts
- 1,514
We have previously gotten these pipes with the hole already drilled. Not sure why not this time. I think the boss has quoted about $2.50 per hole and the customer accepted. Love to do this job at home at that price if it's true. Burr does not matter, as before they had a burr that would take of the end of your finger in not careful. l also think it's an easy job and have calculated that I could just about do 1500 in a day. Not so sure about the other blokes I work with. Had a thought that an Arbor Press with punch and die would work but probably quicker (and cheaper) with a drill press.
Nev.
-
27th Aug 2017, 07:56 PM #6Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Only thing I would suggest is a jig with a drill bush in it, so you can use an ordinary drill and not worry about it wandering - not really an issue for a tooling hole, but it will mean that you don't have to start slow and wait for the drill to bite. If you can find a centre drill of an acceptable diameter you may not even need that. (No. 2 is 3/16" diameter, No. 1 is 1/8").
Michael
-
29th Aug 2017, 09:01 PM #7Senior Member
- Join Date
- Jun 2016
- Location
- Sydney
- Posts
- 283
To be sure, you can use a drill bush with a jobber drill, but you might be better advised to buy a couple of Dormer stub 4 mm coated production drill bits (NOT Chinese and not P&N or Suttons). You only need about 5 mm of travel after all.
Cheers
Roger
Similar Threads
-
drill hole through new shaft to align with pulley taper holes
By MarkBrown in forum METALWORK GENERALReplies: 13Last Post: 9th Sep 2016, 08:20 PM -
How To Drill Accurately Located Holes in Inside Radius of Angle Iron?
By abrogard in forum METALWORK GENERALReplies: 24Last Post: 11th Dec 2012, 09:40 PM -
Drill holes.
By cookie48 in forum METALWORK GENERALReplies: 9Last Post: 5th Aug 2011, 02:18 AM -
Henrob/DHC/Cobra 2000 Oxy Torch
By Jarh73 in forum WELDINGReplies: 10Last Post: 1st Aug 2011, 05:52 PM -
Wanted DHC 2000 welding torch kit
By CJA12005 in forum WELDINGReplies: 13Last Post: 5th Jul 2009, 11:15 AM