    I have a Millard caravan that has been in situ for about 40 years with the rear window facing the setting sun.
    The sealing rubber was severely deteriorated and needed replacing.

    Unfortunately, the inevitable happened during the rubber replacement and a piece of 3 mm polycarbonate was purchased to fill in the hole.

    Got the job done, but the flex in the installed window is alarming !
    I am concerned that a severe wind-storm might simple blow it in.
    The window is 1500 x 500.

    Am I being too concerned ?
    What options could I consider to reduce the risk ?
    Are supplementary strips glued on the inside a practicable fix ?

    Thanks in advance for any comments and/or advice,
    John.

  2. #2
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Pictures would be useful.

  3. #3
    Join Date
    Apr 2009
    Location
    Kingswood
    Posts
    930

    Default

    Sorry, no pictures for a couple of weeks.

    I spoke to the glazier that sold me the rubber beading.
    He said almost impossible to blow the poly window in.
    But, to be sure, just lift the rubber off the poly with a paint scraper and apply some black silicon sealant - use a type that sets.
    He suggested a cloth with kero would clean up any spillage on the poly.

    John.

  4. #4
    Join Date
    Jul 2007
    Location
    sandstone point queensland
    Age
    69
    Posts
    182

    Default

    Quote Originally Posted by electrosteam View Post
    Sorry, no pictures for a couple of weeks.

    I spoke to the glazier that sold me the rubber beading.
    He said almost impossible to blow the poly window in.
    But, to be sure, just lift the rubber off the poly with a paint scraper and apply some black silicon sealant - use a type that sets.
    He suggested a cloth with kero would clean up any spillage on the poly.

    John.
    when i put them in.
    handy to know ,I just picked polycarb windows for all mine on my 1968 viscount and was told that there is no way they will pop out ,still unsure ,will post photos

Similar Threads

  1. Engraving Polycarbonate Coolant/Lubricant
    By electrosteam in forum CNC Forum
    Replies: 6
    Last Post: 19th Mar 2017, 12:53 PM
  2. Plastic Oil Window Repair
    By Bryan in forum METALWORK GENERAL
    Replies: 29
    Last Post: 5th Jan 2011, 02:29 AM
  3. boat window frame
    By swart in forum METALWORK GENERAL
    Replies: 2
    Last Post: 11th Sep 2009, 08:06 PM
  4. No new window?
    By MajorPanic in forum FORUMS INFO, HELP, DISCUSSION & FEEDBACK
    Replies: 12
    Last Post: 11th Aug 2005, 05:53 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •