    I want to make some square holes to hold 6mm or 1/4" HSS. I could file them , but a square push broach sounds more sensible. If any one has a lead on one...

    Michael

  2. #2
    Join Date
    Mar 2014
    Location
    South of Adelaide
    Posts
    1,227

    Default

    If they are through holes I could wire EDM them. PM me if your interested.

  3. #3
    Join Date
    Sep 2011
    Location
    Ballarat
    Age
    65
    Posts
    3,103

    Default

    Is the weekend too late to have a look at what sizes I have.

    Phil

  4. #4
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    Thanks Ash. I'll bear that in mind but as a last resort as there would be several of these.
    No rush - one of a list of many things to look at

    The added bit - In case I've mislead anyone, I have broaches for square keyways. The broach I'm chasing is for making square holes

    Michael
    Last edited by Michael G; 12th Aug 2016 at 07:29 PM. Reason: added a bit

  5. #5
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    Hi Michael,
    Have seen where one was made, from memory a piece of square steel was used and a course thread was cut on it up to about 3/4 of its length. It was then put on a surface grinder and ground down with a taper starting at the threaded end on all 4 sides, the shallow end has the first thread ground off so that it drops in the hole. The whole thing is then heat treated to be able to work. Once that is done, it should be ready to use.
    Found the link //metalworkforums.com/f65/t1993...-square-broach
    Kryn
    Last edited by KBs PensNmore; 12th Aug 2016 at 11:34 PM. Reason: Found the link
    To grow old is mandatory, growing up is optional.

Similar Threads

  1. DIY square broach
    By bob ward in forum METALWORK GENERAL
    Replies: 3
    Last Post: 18th Jun 2016, 11:43 AM
  2. Keyway broach 3/16
    By Greolt in forum METALWORK GENERAL
    Replies: 11
    Last Post: 30th Mar 2016, 09:38 PM
  3. Rota broach annular cutter info
    By Bill13 in forum METALWORK GENERAL
    Replies: 33
    Last Post: 6th Feb 2016, 10:58 AM
  4. Fein magnetic broach core drill
    By Marc in forum METALWORK GENERAL
    Replies: 14
    Last Post: 26th Jan 2015, 09:27 PM
  5. Metric Pulley Keyway Broach
    By electrosteam in forum METALWORK GENERAL
    Replies: 24
    Last Post: 20th Nov 2009, 10:09 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •