Thanks: 0
Needs Pictures: 0
Picture(s) thanks: 0
Results 16 to 19 of 19
Thread: Pressure Gauge
-
19th Feb 2016, 05:03 PM #16Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,562
Or sandwich it between two pieces of say 60 grit sand paper and hammer.
Michael
-
19th Feb 2016, 05:27 PM #17
I realise from the first post that the asked for dimensions were between 3 -6", but a neat way of utilising the brass drain bend would be to use the union nut screwing down a glass lense and behind that, a small gauge to fit in the union (in the pipe). That would look very steampunk-ish I reckon.
-
22nd Feb 2016, 08:12 AM #18Golden Member
- Join Date
- Apr 2009
- Location
- Kingswood
- Posts
- 930
The mates gauge turned out to be an absolutely beautiful 5" brass 800 psi that is still in original wrapping and operating perfectly - I just couldn't bring myself to abandon it tacked onto a pizza oven.
Looked around some antique shops and eventually found the attached 6" for $50.
Press G Arty.JPG
John
-
22nd Feb 2016, 08:10 PM #19Golden Member
- Join Date
- Apr 2009
- Location
- Kingswood
- Posts
- 930
Some good contacts today convinced me that heating swarf in an open topped mould with a torch is a recipe for disaster.
Plan B is to cut the lever shape out of barstock and then to apply the techniques described above.
I wonder if the old tradesman tool markings were really letters shaped out of brass wire laid into grooves, then melted with a torch.
John
Similar Threads
-
Back gear pressure angle
By morrisman in forum THE HERCUS AREAReplies: 9Last Post: 23rd Oct 2014, 10:11 PM -
Pressure Washer Sandblaster
By aussieorchid in forum METALWORK GENERALReplies: 17Last Post: 25th Aug 2013, 01:28 PM -
More compressor help - regulator not supplying appropriate pressure
By 19brendan81 in forum METALWORK GENERALReplies: 14Last Post: 5th Mar 2012, 09:45 PM -
Low pressure gauges?
By nadroj in forum WELDINGReplies: 6Last Post: 27th May 2010, 06:11 PM