New Screwed Backing plate
G'Day All,
After putting up with my lathes (AL300) original 4 jaw chuck backing plate for far too long I decided to do something about it.
The problem being that the fit between the backing plate thread & the lathe spindle nose thread (Ø2.250" x 8 tpi) was to no standard ever used, except by the manufacturer. This resulted in uncontrollable chatter for any reasonable depth of cut & was impossible to part off any size steel workpiece.
As I rarely use a Ø200 4 jaw, I have kept putting this job on the back burner. Now as I need it for a fair bit of turning I have had to do something about it. After acquiring a couple of Ø210 x 45 pieces of mild steel plate I had no more excuses.
Fortunately, the oxy cut surface had been removed by the "supplier" making things a little easier.
DSCF4732.jpg
Rough material setup to start.
DSCF4739.jpg
Plate after rear face turned to size & profile.
DSCF4742.jpg
Plate after bore & register diameter turned to finished size.
DSCF4745.jpg
After screw cutting, the plate being turned to require thickness & the chuck location spigot turned to size.
DSCF4747.jpg
The finished plate after milling ops. for the securing screws.
The chatter caused by the old plate can be seen on the thread finish. The last cut had to chatter didn't it, but the fit is good. The plate has to be screwed onto the spindle nose with a spanner on a chuck jaw for the last 10mm now.
So now, decent cuts & parting off can be achieved.
Regards,
Don.
-
14th May 2018, 08:37 PM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,942
Thanks for the pics and how to, I need to do a couple for my Hercus, when it gets here.
Nice work, even with the chatter. if you wanted to be pedantic, make another to mount the chuck on with the new plate, then remachine the earlier new one.
KrynTo grow old is mandatory, growing up is optional.
-
14th May 2018, 09:54 PM #3
If you need to drive the backplate onto the spindle for the last 3 to 4 turns, you will be locating the chuck on the spindle threads rather than the spindle registers. The concept for a threaded spindle nose was that the chuck/faceplate/backplate threaded onto the spindle freely and with a small clearance in the threads, and that alignment was controlled by the accessory mating with the register and having enough thread clearance to allow the register to true the accessory.
In your case, if the threads mate that tightly that you need to use tools for the last few turns, there will not be enough clearance in the threads for the registration surfaces to do their job.I used to be an engineer, I'm not an engineer any more, but on the really good days I can remember when I was.
-
15th May 2018, 04:52 PM #4Member
- Join Date
- Oct 2017
- Location
- Lismore, NSW
- Posts
- 58
Kryn,
I can put up with the chatter on the thread as I am not making another.
Malb,
The threads are not binding prior to the register faces meeting. I made a master thread gauge years ago when making backing plates for 4 other smaller chucks. The thread tolerance is approx. H7-g6 fit, with the register diameter turned to H7-h6 fit. The use of the spanner is to bring the two diameters together & only a small effort is required.
Regards,
Don.
-
30th Jul 2018, 12:24 PM #5Novice
- Join Date
- Feb 2018
- Location
- Florida, USA
- Posts
- 20
most of the time you can solve the chatter with slower speeds, the unfortunate thing is they will only go so slow.
Nelson
Similar Threads
-
D1-3 Chuck Backing Plate
By Piers037 in forum WANTED TO BUYReplies: 7Last Post: 13th Nov 2017, 09:45 AM -
5" Burnerd chuck backing plate
By ratters in forum WANTED TO BUYReplies: 2Last Post: 8th Jun 2017, 11:05 AM -
Free backing plate from a junked treadmill
By nearnexus in forum METALWORK GENERALReplies: 0Last Post: 7th Mar 2013, 12:38 PM -
Backing plate material
By welder in forum METALWORK GENERALReplies: 17Last Post: 11th Jan 2013, 10:01 AM -
chuck backing plate
By welder in forum THE HERCUS AREAReplies: 5Last Post: 2nd Feb 2010, 05:26 PM