Results 1 to 5 of 5
  1. #1
    Join Date
    Oct 2017
    Location
    Lismore, NSW
    Posts
    58

    Default New Screwed Backing plate

    G'Day All,
    After putting up with my lathes (AL300) original 4 jaw chuck backing plate for far too long I decided to do something about it.
    The problem being that the fit between the backing plate thread & the lathe spindle nose thread (Ø2.250" x 8 tpi) was to no standard ever used, except by the manufacturer. This resulted in uncontrollable chatter for any reasonable depth of cut & was impossible to part off any size steel workpiece.
    As I rarely use a Ø200 4 jaw, I have kept putting this job on the back burner. Now as I need it for a fair bit of turning I have had to do something about it. After acquiring a couple of Ø210 x 45 pieces of mild steel plate I had no more excuses.
    Fortunately, the oxy cut surface had been removed by the "supplier" making things a little easier.

    DSCF4732.jpg
    Rough material setup to start.

    DSCF4739.jpg
    Plate after rear face turned to size & profile.

    DSCF4742.jpg
    Plate after bore & register diameter turned to finished size.

    DSCF4745.jpg
    After screw cutting, the plate being turned to require thickness & the chuck location spigot turned to size.

    DSCF4747.jpg
    The finished plate after milling ops. for the securing screws.

    The chatter caused by the old plate can be seen on the thread finish. The last cut had to chatter didn't it, but the fit is good. The plate has to be screwed onto the spindle nose with a spanner on a chuck jaw for the last 10mm now.
    So now, decent cuts & parting off can be achieved.
    Regards,
    Don.

  2. #2
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    Thanks for the pics and how to, I need to do a couple for my Hercus, when it gets here.
    Nice work, even with the chatter. if you wanted to be pedantic, make another to mount the chuck on with the new plate, then remachine the earlier new one.
    Kryn
    To grow old is mandatory, growing up is optional.

  3. #3
    Join Date
    Oct 2007
    Location
    Alexandra Vic
    Age
    69
    Posts
    654

    Default

    If you need to drive the backplate onto the spindle for the last 3 to 4 turns, you will be locating the chuck on the spindle threads rather than the spindle registers. The concept for a threaded spindle nose was that the chuck/faceplate/backplate threaded onto the spindle freely and with a small clearance in the threads, and that alignment was controlled by the accessory mating with the register and having enough thread clearance to allow the register to true the accessory.
    In your case, if the threads mate that tightly that you need to use tools for the last few turns, there will not be enough clearance in the threads for the registration surfaces to do their job.
    I used to be an engineer, I'm not an engineer any more, but on the really good days I can remember when I was.

  4. #4
    Join Date
    Oct 2017
    Location
    Lismore, NSW
    Posts
    58

    Default

    Kryn,
    I can put up with the chatter on the thread as I am not making another.

    Malb,
    The threads are not binding prior to the register faces meeting. I made a master thread gauge years ago when making backing plates for 4 other smaller chucks. The thread tolerance is approx. H7-g6 fit, with the register diameter turned to H7-h6 fit. The use of the spanner is to bring the two diameters together & only a small effort is required.
    Regards,
    Don.

  5. #5
    Join Date
    Feb 2018
    Location
    Florida, USA
    Posts
    20

    Default

    most of the time you can solve the chatter with slower speeds, the unfortunate thing is they will only go so slow.
    Nelson

Similar Threads

  1. D1-3 Chuck Backing Plate
    By Piers037 in forum WANTED TO BUY
    Replies: 7
    Last Post: 13th Nov 2017, 09:45 AM
  2. 5" Burnerd chuck backing plate
    By ratters in forum WANTED TO BUY
    Replies: 2
    Last Post: 8th Jun 2017, 11:05 AM
  3. Free backing plate from a junked treadmill
    By nearnexus in forum METALWORK GENERAL
    Replies: 0
    Last Post: 7th Mar 2013, 12:38 PM
  4. Backing plate material
    By welder in forum METALWORK GENERAL
    Replies: 17
    Last Post: 11th Jan 2013, 10:01 AM
  5. chuck backing plate
    By welder in forum THE HERCUS AREA