    Default DIY Brass Scriber, Clickspring Inspired

    HI all, first post here. I posted this little project over on the Garage Journal forum and Grahame Collins suggested I come and check out this forum, so here I am.

    I watched a youtube video some time ago by and Australian machinist and clock maker that goes by the name of Clickspring, if you haven't seen any of his videos then do yourself a favour and look them up, he is brilliant.


    Anyway one of his videos is for a brass scriber which I have based this project on, mine is made slightly differently because I only used what I had lying around to get the job done.


    First off I needed some brass rod, which I didn't have, but I did have a couple of old tap spindles that were brass





    In the Video Chris used a sewing needle for his scriber tip, I didn't have any of those either, but I do have a heap of very small thread taps that I got in a lot deal off Ebay some time ago, they are really small and SAE so I will never use them, except for scriber tips





    I needed to join the 2 spindles together, and obviously that would leave a join in the middle of my scriber, rather than try and hide it I thought I would highlight it, so I used a piece fo 6mm Aluminium in the centre as a contrast to the brass. It probably didn't contrast as much as I would have liked, but it turned out fine none the less. I used some 6mm all thread in the join, the tap spindles already had a hole from where the washer fitted in, so I didn't even need to drill, just tap the thread.





    Then screw it all together with some Loctite to hold it.





    Then it was into the lathe to turn it to size which is a nominal 9mm diameter, diam is not critical so I didn't even measure it. then taper the end and put some grooves in the handle for extra grip, sorry forgot to take photos whilst machining.


    I drilled a hole in one end for the thread tap to be inserted, it was an interference fit so I had to hammer it home making it a nice tight fit. I then shaped and sharpened the tip on the lathe using a flap disc on the angle grinder.





    And the end result.











    Cheers Andrew

  2. #2
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Hi AJ,

    Welcome to our MetalWork Forums,

    Thank you for your post on your scriber.The notion of using an old tap spindle in lieu of a new bit of expensive and hard to get material (at least in my neck of the woods) is an awesome idea.

    The project certainly hooks my attention as I do have an interest in making small metalworking handtools and because it is an excellent example of the repurposing of a usually discarded or scrapped item and then transforming it into a tool which is useful but also visually appealing.
    Please keep an eye out for a PM in which I'll send some links to help you understand and operate within the forum.

    Clickspring is mentioned here in our forum on a regular basis.

    Again a very big welcome

    Grahame

  3. #3
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Great job. I also like repurposing stuff and have used brass plumbing fittings in lost of my projects.

  4. #4
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Nice job. I would never have believed that scriber came out of two tap spindles if I hadn't seen the progress shots.
    Chris

  5. #5
    Join Date
    May 2009
    Location
    Canberra
    Posts
    1

    Default

    Quote Originally Posted by AJ. View Post
    HI all, first post here. I posted this little project over on the Garage Journal forum and Grahame Collins suggested I come and check out this forum, so here I am.

    I watched a youtube video some time ago by and Australian machinist and clock maker that goes by the name of Clickspring, if you haven't seen any of his videos then do yourself a favour and look them up, he is brilliant.


    Anyway one of his videos is for a brass scriber which I have based this project on, mine is made slightly differently because I only used what I had lying around to get the job done.


    First off I needed some brass rod, which I didn't have, but I did have a couple of old tap spindles that were brass





    In the Video Chris used a sewing needle for his scriber tip, I didn't have any of those either, but I do have a heap of very small thread taps that I got in a lot deal off Ebay some time ago, they are really small and SAE so I will never use them, except for scriber tips





    I needed to join the 2 spindles together, and obviously that would leave a join in the middle of my scriber, rather than try and hide it I thought I would highlight it, so I used a piece fo 6mm Aluminium in the centre as a contrast to the brass. It probably didn't contrast as much as I would have liked, but it turned out fine none the less. I used some 6mm all thread in the join, the tap spindles already had a hole from where the washer fitted in, so I didn't even need to drill, just tap the thread.





    Then screw it all together with some Loctite to hold it.





    Then it was into the lathe to turn it to size which is a nominal 9mm diameter, diam is not critical so I didn't even measure it. then taper the end and put some grooves in the handle for extra grip, sorry forgot to take photos whilst machining.


    I drilled a hole in one end for the thread tap to be inserted, it was an interference fit so I had to hammer it home making it a nice tight fit. I then shaped and sharpened the tip on the lathe using a flap disc on the angle grinder.





    And the end result.











    Cheers Andrew
    Nice work. I use worn chainsaw chain files - they are long enough to grind both a pointed & a chisel end. Only a couple of minutes work.

    Sent from my CPH1701 using Tapatalk

  6. #6
    Join Date
    Feb 2018
    Location
    Loxton
    Age
    54
    Posts
    37

    Default

    Thanks guys, lucky I took progress shots as evidence hey

    I probably have heaps of other old projects and some current major projects that might interest you guys, I will post some more stuff up when I get a chance.

    Cheers Andrew

  7. #7
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,658

    Default

    I have been entertaining the idea of making a scriber since using buy commercial one as a pry bar proved fatal, I know just where a couple of old tap spindles are hiding
    the notion of using old tap spindles never would have entered my head

  8. #8
    Join Date
    Sep 2012
    Location
    York, North Yorkshire UK
    Posts
    6,477

    Default

    Hi Guys,

    Nice work on the scriber.

    I regularly raid the local scrap yard for bits and pieces of material, and sometimes find bits of useful gear as well !
    Best Regards:
    Baron J.

  9. #9
    Join Date
    Feb 2009
    Location
    moonbi nsw Aus
    Age
    69
    Posts
    364

    Default

    Yep certainly agree with the methodology behind the making of the scriber. Using the tap, I would have tapped the hole using the said tap, screwed in in tight then sharpened it to suit. That way if the steel part was to have a mishap you could unscrew it and replace it with another tap and reshape.....just a thought
    Just do it!

    Kind regards Rod

  10. #10
    Join Date
    Feb 2018
    Location
    Loxton
    Age
    54
    Posts
    37

    Default

    Quote Originally Posted by chambezio View Post
    Yep certainly agree with the methodology behind the making of the scriber. Using the tap, I would have tapped the hole using the said tap, screwed in in tight then sharpened it to suit. That way if the steel part was to have a mishap you could unscrew it and replace it with another tap and reshape.....just a thought
    Yeah well that would have been the smart way to go about it, but I never claimed to be smart

    Cheers Andrew

  11. #11
    Join Date
    Feb 2018
    Location
    Florida, USA
    Posts
    20

    Default

    was the pics removed or am I missing something?
    Nelson

  12. #12
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    Quote Originally Posted by Nrcollar View Post
    was the pics removed or am I missing something?
    Nelson
    I think those pics may be from an external source and something beyond the control of this Forum has occurred.

    Possibly some of our members may have been impressed enough to copy the pics and might post them for us.

    < EDIT> I have completed a Google search and found 2 other forums where it was posted and the same has occurred- No pics

    I found the following in Google images -this was one of the pics in the original article.

    Grahame


    Scriber from brass tap spindle.jpg

  13. #13
    Join Date
    Feb 2018
    Location
    Florida, USA
    Posts
    20

    Default

    I believe Chris would very satisfied with you gorgeous tool.
    Wonderful job, enjoy you new tool.
    Nelson

Similar Threads

  1. what rods for thin brass to brass ??
    By Mathuranatha in forum WELDING
    Replies: 7
    Last Post: 23rd Nov 2020, 08:17 PM
  2. VICTORIA Brass Flat Bar Assorted Sizes & 1/4" SWB Threaded Rod & 260 Carbide Brass Sheet
    By thumbsucker in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 7
    Last Post: 18th Mar 2013, 03:36 PM
  3. Spitfire-inspired chair
    By tiger_ted in forum METALWORK GENERAL
    Replies: 11
    Last Post: 20th Feb 2013, 03:38 PM
  4. Shy scriber
    By Steamwhisperer in forum METALWORK GENERAL
    Replies: 15
    Last Post: 31st Jan 2012, 01:07 PM
  5. brass
    By tanii51 in forum METALWORK GENERAL
    Replies: 3
    Last Post: 22nd Aug 2009, 09:21 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •