Hydraulic suction fitting
As part of my hydraulic log splitter project i needed a fitting for the suction side of the pump. The pump uses UN (O) fittings on both the suction and pressure sides. UNO fittings use an o-ring to create a seal rather than rely on the thread, they dont seem to be very common but not unobtainable. The suction port has a 1-5/8" UNO fitting and i needed one that went to a 1-1/2" barb fitting to take the suction hose. These can be ordered through my local hydraulic supplier but at $65 for the fitting i figured id make it myself.
Ended up working really well. Being a 12 tpi thread on my metric lathe, as usual i left the half nuts engaged. I used a part off tool to make a run out groove which also served as the o-ring groove.
The o-ring seats in a groove on the female side and so the fitting seats hard onto the female compressing the o-ring a defjned amount.
The biggest issue was the material. I asked for and purchased a piece of 50mm MS bright but there is no way its MS. It was very tough, machined beautifully with tc tooling but was tough as all.
I also machined some flats to aid in tightening it on.
Anyway. Happy withvthe result and saved some coin.
Cheers.
Simon
Sent from my SM-G900I using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
23rd Jan 2018, 06:20 PM #2Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,225
Good job. UNO is a pretty standard port size on valves and pumps. Normally you would have a UNO to JIC nipple in the port, then JIC ends on the hose. I would recommend using the wide style hose clamps with the bolt, not the more common worm drive type, it will hold and seal better.
-
23rd Jan 2018, 08:38 PM #3Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Thanks Snapatap. OK so it's more common than I realise. I'm not in the hydraulics game so I have a lot to learn.
Yes, the pressure side has a un(o) to JIC-12 fitting that I purchased. All the other fittings in the pressure system use JIC-12 with 3/4" hose. The return is 1".
Thanks for the advice on the hose clamps.
Cheers,
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
23rd Jan 2018, 09:06 PM #4Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,216
Very nice work, only thing I would have done differently would been to have made the end barbed. Not that it matters on a suction.
Gold, the colour of choice for the discerning person.
-
24th Jan 2018, 08:16 AM #5Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Thanks RC. I did think about pulling out my radius turner to put a rounded barb on the end but as you said, in suction it's hardly going to come off. The hose is already a snug fit and the hose slides on 2". So yes, a bought one would have a barb but I think I'll get away with it.
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
15th Apr 2018, 04:44 AM #6Most Valued Member
- Join Date
- Oct 2010
- Location
- melbourne, laverton
- Posts
- 1,910
Nice. I've used a fair bit a . 45deg double male fitting . The same o ring set up.
On the other end a piece of threaded pipe suitable size for suction hose.i prefer yours.
-
15th Apr 2018, 11:17 AM #7Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Thanks. Not shown in the photos, I also added a tapped hole in one of the square sections for a temperature sender. It will measure the hydraulic oil temp before it enters the pump.
Apparently the oil is good to about 100 degrees, however the seals in the pump (according the the manufacturer) are only rated to 80 degrees. So I figured it was more important to monitor the temp going into the pump and not the temp of the oil in the return line.
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
15th Apr 2018, 07:06 PM #8Most Valued Member
- Join Date
- Oct 2010
- Location
- melbourne, laverton
- Posts
- 1,910
Wow rdmp sender in your of splitter.
I think if you have a big enough tank it won't go near those temps.
-
16th Apr 2018, 12:54 PM #9Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
I hope so but its all new to me so not sure what temps the oil will reach during an average run of couple hours splitting. The resevoir is about 70 litres and a 39 GPM pump.
It was only a cheapie gauge on ebay so figured why not since im making it!!
Sent from my SM-G900I using TapatalkGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
Similar Threads
-
Fitting Reg to bottle
By DSEL74 in forum WELDINGReplies: 5Last Post: 14th Mar 2016, 10:07 AM -
welding to hydraulic ram
By jatt in forum WELDINGReplies: 14Last Post: 15th Nov 2015, 09:55 PM -
Fitting a DRO to my lathe
By tbonesmith in forum METALWORK GENERALReplies: 2Last Post: 26th Mar 2014, 12:15 PM -
Hydraulic ram
By GSRocket in forum METALWORK GENERALReplies: 8Last Post: 6th Oct 2012, 10:19 AM -
Fitting an ER 40 to an AL320G
By barkersegg in forum METALWORK GENERALReplies: 16Last Post: 11th Nov 2010, 08:21 AM