    Hi.
    Can anyone help with a supplier of glass tube for a drip oiler.. ?
    Ken.

  2. #2
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,561

    Default

    What diameter do you need? I have two pieces 1 1/4" (I think) left over from when converted some oil drippers to 1" size.

    Michael

  3. #3
    Join Date
    Nov 2008
    Location
    Brisbane Australia
    Posts
    122

    Default

    Hi.
    Try Labglass at Windorah St at Stafford.
    Jim.

  4. #4
    Join Date
    Jul 2010
    Location
    Brisbane
    Posts
    143

    Default

    size required is 38mm dia x 35mm high.
    Cheers .. Ken.

  5. #5
    Join Date
    Sep 2008
    Location
    texas, queensland
    Posts
    248

    Default

    i used polycarb or perspex not sure which in solid rod and just bored it out . then polished it with wet and dry then toothpaste didnt take long to do .
    'If the enemy is in range, so are you.'

  6. #6
    Join Date
    Jul 2008
    Location
    near Warragul, Victoria
    Posts
    3,726

    Default glass

    Remember when people used to make glass drinking cups out of beer bottles ? Back when we made stuff !

    Go to your local op shop and buy some drinking glass of the correct diameter , scribe a line around the glass and heat up with metho, then cool it under the tap , takes a little practice to perfect the method.

    Smooth the edges off with glass paper or a linisher and that's it . Glass looks so much better than perspex in a oiler .

  7. #7
    Join Date
    Sep 2008
    Location
    texas, queensland
    Posts
    248

    Default

    mine was for a model hit and miss engine it was about 5/8" or 3/4 " diameter from memory .
    'If the enemy is in range, so are you.'

  8. #8
    Join Date
    Feb 2018
    Location
    Florida, USA
    Posts
    20

    Default

    Ken
    My wife is a diabetic and takes insulin. The insulin bottles are glass a little larger than a quarter and about 1.25 tall. Cut the top and bottom off makes a nice glass cylinder that holds about .5 oz of oil.
    Good luck
    Nelson

  9. #9
    Join Date
    Sep 2016
    Location
    Canberra
    Posts
    88

    Default

    Quote Originally Posted by texx View Post
    i used polycarb or perspex not sure which in solid rod and just bored it out . then polished it with wet and dry then toothpaste didnt take long to do .

    That Sir is a fantastic idea!
    I will try that with my broken lathe dirp oiler!

  10. #10
    Join Date
    Feb 2018
    Location
    Florida, USA
    Posts
    20

    Default

    Another thing that is available almost every where is test tubes. You can buy all different sizes.
    Check out this site. I think you can get any size you would want:
    https://www.indigoinstruments.com/glassware/test_tubes/

    Good luck and keep up on the progress.
    Nelson

Similar Threads

  1. Drip oilers
    By morrisman in forum METALWORK PROJECTS
    Replies: 4
    Last Post: 7th Jul 2016, 09:46 PM
  2. Need a New Myfrod Drip Tray
    By wheelinround in forum METALWORK GENERAL
    Replies: 15
    Last Post: 30th Jun 2016, 07:19 PM
  3. N.S.W. Bench and drip tray for small lathe.
    By clear out in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 5
    Last Post: 20th Apr 2013, 05:51 PM
  4. Drip or wick oilers?
    By Old Hutcho in forum METALWORK GENERAL
    Replies: 8
    Last Post: 9th Oct 2012, 07:44 PM
  5. Drip tray for lathe
    By snowyskiesau in forum METALWORK GENERAL
    Replies: 13
    Last Post: 4th Feb 2008, 08:23 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •