Needs Pictures: 0
Results 76 to 77 of 77
-
16th Jun 2017, 05:50 PM #76Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,541
I've gotten most of the grinder back together now and it looks much better than the ratty unpainted photos, so just for bragging rights...
Lights were on special at the local lighting shop. They are wired in such that when power is present they are on.
P1040109 (Small).JPG
right and left sides with belt arrangement
P1040112 (Small).JPG P1040111 (Small).JPG
Completed clutch assembly and the horribly complex brake pad.
P1040110 (Small).JPG P1040115 (Small).JPG
Still need to derust the tension rollers for the work head drive and sort out some of the accessories, as well as some minor tidying op of wiring and so on.
Michael
-
16th Jun 2017, 05:57 PM #77Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
That came up real neat Michael.
It's nice when you can call a project "finished".
Cheers,
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
Similar Threads
-
Jones - Shipman Tool And Cutter Grinder
By KBs PensNmore in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 0Last Post: 20th Sep 2015, 01:31 AM -
Jones - Shipman Tool And Cutter Grinder
By KBs PensNmore in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 0Last Post: 18th Sep 2015, 01:33 AM -
Jones and Shipman pics for Bob (Krisfarm)
By Steamwhisperer in forum METALWORK GENERALReplies: 54Last Post: 9th Feb 2015, 02:29 PM -
Suitable motor for Jones & Shipman Drill
By krisfarm in forum METALWORK GENERALReplies: 6Last Post: 29th Aug 2014, 10:57 AM -
Jones and Shipman drill press 1932
By jgforsberg in forum METALWORK GENERALReplies: 5Last Post: 26th Jun 2012, 06:15 PM