I started building a new eye bender on Monday unfortunately unforeseen unfortunate events have & will prevent me from finishing for a while.
Adjustment pin holes for the clamping bar. 1/2" drilled on the Denbigh. Drilled 2up back to back combined thickness 20mm
Mock assembly
1" SHS to be bolted to the base so it can be held in the vice. My previous one had angle iron but some of the old post vices are too worn to hold well on such a thin section.
Drilling the main arm for the die pins.
I timed the actual drill time, set up and alignment not included. It takes the Denbigh 4:31.28 minutes to put a through hole in. So if you add up all those holes and multiply by 4 1/2 min it takes a while.
…..Live a Quiet Life & Work with your Hands
-
16th Apr 2017, 10:44 PM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Thanks for the pics. Look forward to seeing it in operation.
KrynTo grow old is mandatory, growing up is optional.
-
16th Apr 2017, 10:54 PM #3
what is a eye bender ?
-
16th Apr 2017, 11:12 PM #4
An eye bender is used to bend solid rod or bar into round loops.
Good for doing eyes on the end of hooks etc.…..Live a Quiet Life & Work with your Hands
-
29th Apr 2017, 06:47 PM #5
Eye bender Build
Been going stir crazy, So a friend came around to supervise me in the shed today and make sure I didn't do too much. I did some drilling, tapping and welding and made the bender look more like a bender than a pile of metal bits.
The vide block bolted on.
The body and arm are all finished.
Now just the clamp lever to go.
A few hrs in the shed and I'm exhausted just laying on the couch trying not to fall a sleep.…..Live a Quiet Life & Work with your Hands
-
30th Apr 2017, 12:08 AM #6
Good to have friend's that can help
Sent from my SM-G935F using Tapatalk
Similar Threads
-
Roller Bender Build
By DSEL74 in forum METALWORK GENERALReplies: 14Last Post: 9th Mar 2017, 08:37 AM -
WTB: flat bar bender
By meadow street in forum METALWORK GENERALReplies: 10Last Post: 16th Aug 2015, 05:50 PM -
help me build a basic flat build bed trailer for my kayaks
By gros21 in forum TRAILERS & OTHER FABRICATED STUFFReplies: 7Last Post: 13th Oct 2011, 08:47 AM -
Trailer - to build or not to build
By motegi in forum TRAILERS & OTHER FABRICATED STUFFReplies: 17Last Post: 6th May 2009, 03:07 PM -
Rod bender
By Andy Mac in forum METALWORK GENERALReplies: 4Last Post: 4th Aug 2008, 10:47 PM