Page 3 of 4 FirstFirst 1234 LastLast
Results 31 to 45 of 50
  1. #31
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    470

    Default

    Got the saddle on today and done some tests on the oil system all good and now stated work on the tail stock.

    Resize of IMG_5932.jpgResize of IMG_5933.jpgResize of IMG_5935.jpgResize of IMG_5937.jpgResize of IMG_5942.jpgResize of IMG_5941.jpgResize of IMG_5940.jpgResize of IMG_5945.jpgResize of IMG_5946.jpg
    Attached Images Attached Images

  2. #32
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    470

    Default

    I had to drill holes in the tailstock base plate to get these rollers out. And clean up the compound and quick change tool holder and adjusted all the gibs, will check it again when i level out the lathe.Resize of IMG_5955.jpgResize of IMG_5947.jpgResize of IMG_5948.jpgResize of IMG_5952.jpgResize of IMG_5953.jpgResize of IMG_5954.jpg

  3. #33
    Join Date
    Aug 2008
    Location
    near Rockhampton
    Posts
    6,218

    Default

    I would leave those rollers out. They do not achieve much. My 10EE had a similar setup but with balls. The idea is you unlock the tailstock and the spring loaded rollers lift the tailstock and it runs along the rollers, stopping wear. They forgot that over time they sieze up and just wear flats and wear out the tailstock bed ways.
    Gold, the colour of choice for the discerning person.

  4. #34
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    470

    Default

    Yeah i was thinking of leveing them out, i have some bakelite material somewhere or i could use some Igus material. The tailstock is very heavy.

  5. #35
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    470

    Default

    Work on the lathe has slowed down a bit, waiting for a piece of bakelite rod to arrive then i can finish off the tailstock repair. Cleaned up the back panels and bolted them in back in place, will see if i can get the ammeter gauge repared or find a replacement. Working on the felt wiper holders at the moment.

    Resize of IMG_5970.jpgResize of IMG_5969.jpgResize of IMG_5962.jpgResize of IMG_5965.jpgResize of IMG_5966.jpgResize of IMG_5967.jpgResize of IMG_5968.jpg

  6. #36
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    470

    Default

    Been doing a bit of work on the lathe, not much as we are getting close to Xmas, so lots of preparation jobs to be done for Xmas. I took out the coolant pump and clean out that section of the tank were the pump sits, lots of flaky paint was coming off need to get get as much of that paint off so it wont block the pump, it had wire mesh sitting under the pump with a hose clamp don't know if that was factory fitted I pulled apart the 3 jaw scroll chuck for cleaning, very worn out scroll gear will need a replacement chuck in the future.

    Resize of IMG_6007.jpgResize of IMG_6001.jpgResize of IMG_6006.jpgResize of IMG_6002.jpgResize of IMG_6004.jpgResize of IMG_6005.jpg

  7. #37
    Join Date
    Mar 2014
    Location
    South of Adelaide
    Posts
    1,227

    Default

    I wouldn't be too worried about the wear on the scroll gear. It would have taken 30 years of workshop abuse to get to that stage, I doubt it will get any worse. If the chuck run out isn't too bad I wouldn't bother replacing it.

  8. #38
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    470

    Default

    Yeah 30 + years of abuse, will still use it and will get a new chuck latter on. Have started cleaning up the 4 jaw chuck at the moment something is not right with this chuck, will give a update latter today.

  9. #39
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    470

    Default

    Pulled apart the 4 jaw chuck, was hard to unscrew each jaw out of the chuck clean all the parts up and done a test fit before assembly. All the jaws got stuck number 3 jaw almost went all the way in, does anyone know were i can get this chuck repaired or should i get a replacement chuck

    Resize of IMG_6011.jpgResize of IMG_6010.jpg

  10. #40
    Join Date
    Jul 2016
    Location
    Melbourne
    Age
    35
    Posts
    1,522

    Default

    Will the jaws go in if you try them in different slots? are they numbered by the factory, some more detailed photos of the chuck jaw slots and screws might help. In terms of fixing the thing, you are on your own I would say (with us around though )

    my guess would be something like although the jaws are in the right slots the screws themselves have been mixed around, some hi-spot blue or a sharpie might let you see what kind of contact is being made.

    If you need another lathe to fix the screws happy to volunteer my time and machine.

    Ralph

  11. #41
    Join Date
    Oct 2011
    Location
    Norwood-ish, Adelaide
    Age
    59
    Posts
    6,562

    Default

    If they were in there to start with then it can not be all bad - in fact it's good as it looks like there is not much wear there. From your photos it looks like you have no lubrication between the jaws and the chuck body, and that the screws are not in. For a tight fit you would have better success with both I think.
    Check both the jaws and the part they run in for burrs. It may be in the past something has dinged part of the chuck slightly. Emery wrapped around a file or flat block should be enough to take off the high points.

    Michael

  12. #42
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    470

    Default

    Quote Originally Posted by Michael G View Post
    If they were in there to start with then it can not be all bad - in fact it's good as it looks like there is not much wear there. From your photos it looks like you have no lubrication between the jaws and the chuck body, and that the screws are not in. For a tight fit you would have better success with both I think.
    Check both the jaws and the part they run in for burrs. It may be in the past something has dinged part of the chuck slightly. Emery wrapped around a file or flat block should be enough to take off the high points.

    Michael
    Yeah i know what you mean, the chinese lathe i had the chuck was very hard to turn with the chuck key, i found out the scroll gear had some warpage due to over tightening of the chuck me thinks I got some flat block brass and stuck emery cloth on and gave a bit of sanding has fix it, not prefect but once i start working with the lathe will put the 4 jaw chuck to work and will see if it wears in a bit and make it more user friendly.

  13. #43
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    470

    Default

    Quote Originally Posted by caskwarrior View Post
    Will the jaws go in if you try them in different slots? are they numbered by the factory, some more detailed photos of the chuck jaw slots and screws might help. In terms of fixing the thing, you are on your own I would say (with us around though )

    my guess would be something like although the jaws are in the right slots the screws themselves have been mixed around, some hi-spot blue or a sharpie might let you see what kind of contact is being made.

    If you need another lathe to fix the screws happy to volunteer my time and machine.

    Ralph
    Hi Ralph,
    Thanks for the offer mate. I tried using different slots still have the same problem, the jaws are fine and the screws are prefect it's the chuck housing. But i have fix the problem using some emery cloth stuck on a brass flat and just gave the slots a bit of sanding, a good 45 minutes on one slot three more to go.

  14. #44
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    470

    Default

    Some photos of what i have done for this year. I got a second hand pratt burnerd chuck to replace the worn out one, only problem with this one no reverse jaws Panted the sides of the coolant tank and replace the hose as the other hose was hard as a rock, and fitted the chip guard back on will do some mods to the guard in the new year. Got my first quote to run a three phase line to the garage $4,026 including GST. I'll get some more quotes next year.

    Resize of IMG_6022.jpgResize of IMG_6021.jpgResize of IMG_6023.jpgResize of IMG_6024.jpgResize of IMG_6027.jpg

  15. #45
    Join Date
    Oct 2016
    Location
    Melbourne
    Posts
    470

    Default

    OK new year update on the lathe, had new rollers made up out of some bakelite rod for the tail stock. I'm thinking i could of use brass or bronze for the rollers, but this will do for now and i want to make new roller carriers as well.
    At last got the three phase line installed , three electrical contractors to do the job was a lot to do. Now got to wait for the truck appointment to hook up three phase power witch may take two weeks won't be long know and i can do some test on the machine.

    Resize of IMG_6064.jpgResize of IMG_6062.jpgResize of IMG_6076.jpgResize of IMG_6077.jpgResize of IMG_6078.jpgResize of IMG_6080.jpg

Page 3 of 4 FirstFirst 1234 LastLast

Similar Threads

  1. Metal lathe Identification and Sloppy Input Clutch Repair
    By brianwynn in forum METALWORK GENERAL
    Replies: 16
    Last Post: 10th Jul 2016, 09:03 PM
  2. lathe Identification and Sloppy Input clutch repair ?
    By brianwynn in forum ANTIQUE AND VINTAGE MACHINERY
    Replies: 4
    Last Post: 9th Jul 2016, 12:02 AM
  3. Elliott Lathe bed clean
    By argeng in forum METALWORK GENERAL
    Replies: 20
    Last Post: 22nd May 2013, 03:46 PM
  4. Lathe tailstock repair (retapping grub screw)
    By HSS in forum METALWORK GENERAL
    Replies: 2
    Last Post: 12th Sep 2012, 06:11 PM
  5. Hercus lathe, clean bed ways?
    By neksmerj in forum METALWORK GENERAL
    Replies: 3
    Last Post: 30th Dec 2007, 12:53 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •