18th Dec 2017, 10:59 PM #1
shot peening
Does anyone have experience of shot peening engine parts?
I have a NOS set of old Morris 4 ring pistons, a aftermarket brand . These are heavy pistons which I think means they have a high iron content. These type of pistons normally have a thin tin coating , the tin coating aids the running in process. In this case the tin has come away or fallen off after many years of storage.
Years ago I shot peened a set of used chevy iron pistons , I actually used a fine sand but I think the professionals use glass or ceramic beads . Anyway the chevy pistons have been running without any problems. I am wondering If I should do the same with these Morris pistons?
piston.jpg
-
19th Dec 2017, 07:53 AM #2
Hi Morrisman,
You are not going to leave us all hanging, are you? Let the other boot drop.
What was the long-term result from shot peening the Chevy pistons?
The sand once used in commercial sandblasting was pretty much outlawed by the various safety bodies. Silicosis was a very big safety issue at the time.
The old machinery department came into the refinery and the sandblaster crew had to change to a garnet based pellet.
I recently purchased a sandblasting cabinet and the grit that came with it appears to be rutile which is as slow as buggery but gives a nice fine finish.
Is running in that style of motor an issue ,these days, given vehicles run up to 15,000kms to the first oil change,or at least my Hyundai does?
Or is the Morry motor a diffrent kettle of fish?
Grahame
-
19th Dec 2017, 12:14 PM #3
hi Grahame
I think they peen engine parts because it relieves surface tension, or something like that . I know they do it to con rods to minimise any potential fatigue cracks. I am not a auto engineer by any standard.
The tiny little indentations also hold oil .
The chevy pistons are still running without any problems , fingers crossed.
The old Morris engine is a 1930's era motor.
-
19th Dec 2017, 12:34 PM #4
Hi Morrisman,
The Morris pistons should not be a drama then. I think the clearances and the quality of the oils these days are the difference.
The pistons remind me of a Chrysler straight 8 engine I saw stripped down.
My uncle who owned it reckoned it would pull a caravan up a cliff face, but being a big slow revving deep skirted long stroke motor I understand it would be very torquey.
Grahame
-
19th Dec 2017, 12:57 PM #5Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,666
I think you might be getting shot peening confused with bead blasting. Proper shot peening is typically done with metal (usually steel) shot and in my experience done for fatigue resistance as you suggested. The time/coverage and intensity of the process is quite closely controlled to ensure that the part receives the required amount of peening. Do a search on Almen strips for more info
Bead blasting using glass bead or similar is mainly a cleaning process, but does produce some compression of the part surface - enough to cause distortion on thin flat panels but generally no issue on more solid parts. We used quite a bit of glass bead blasting for corrosion removal on aircraft.
IMO there'd be no point shot peening those parts, but using glass bead or similar to clean them would be fine.
Steve
-
19th Dec 2017, 05:33 PM #6Golden Member
- Join Date
- Apr 2008
- Location
- NSW
- Posts
- 537
Shot peening was done in my day to mainly conrods not pistons . Sand would just clean them nothing else. Shot means hard steel balls sometimes tungsten and the idea is it shallow cold forges the surface reducing forging stress at the surface that could lead to the start of fatigue cracks . Only iron , steel and titanium rods would get any benefit . Alloy rods it would be a waste of time and money . Polishing alloy rods would be more useful .
The volume of a pizza of thickness 'a' and radius 'z' is given by pi z z a.
-
20th Dec 2017, 08:59 AM #7
The above is the gist of Morrismans inquiry as I see it.
Morrisman wants to remove, what is now a partial tin coating of these pistons.
The blasting / peening will do this.The light peening action will also assist in retaining oil during the run in .
I don't see a problem with that.
Grahame
-
23rd Dec 2017, 10:01 AM #8Senior Member
- Join Date
- Dec 2010
- Location
- Syd
- Posts
- 492
I'd probably have a word to this bloke if there's nobody you know down that way MT&C Engineers - Home Page always found him helpful with ndt, peening and friction questions.
I've been using plastic shot on some stuff like that, start to have some concerns about the ring lands if over-enthusiastic.
Similar Threads
-
One shot
By sossity in forum METALWORK GENERALReplies: 3Last Post: 23rd Dec 2016, 10:10 AM -
One shot oiler
By Oldneweng in forum METALWORK GENERALReplies: 33Last Post: 15th Jan 2016, 10:17 AM -
Peening a Sliding Handle
By bwal74 in forum METALWORK GENERALReplies: 3Last Post: 30th Dec 2013, 05:21 PM -
I shot the sheriff but I didn't shoot the deputy
By Machtool in forum METALWORK GENERALReplies: 19Last Post: 4th Apr 2013, 05:24 PM -
One shot lube systems for Mills and Lathes
By markjaffa in forum METALWORK GENERALReplies: 91Last Post: 6th Jan 2011, 12:49 AM