    Default Different repair of a Cast Iron Head

    Saw an interesting process on a British show, Car SOS, on Friday Night 3rd Feb. around midnight. A cylinder head had a crack in the water jacket on top of the head, where there is a raised section like a pipe that goes to the radiator, that had the crack in it.
    How it was done was called a cold welding process, that entailed cutting out the cracked section and replacing it with another piece of cast metal, this was hammered in, then cut across the joins, clips inserted and a special type of screw inserted.
    The whole repair section was then filed flush, to look very similar to the finished head.
    Tried to find a You Tube Video of it but all entailed a welder.
    To grow old is mandatory, growing up is optional.

  2. #2
    Join Date
    Aug 2010
    Location
    Near Bendigo, Victoria, AUS
    Age
    72
    Posts
    3,104

    Default

    I think its called "stitching".
    Here is a training video of one of the many commercial processes:
    https://www.youtube.com/watch?v=Pq0wfU4ZaKk
    Cheers, Joe
    retired - less energy, more time to contemplate projects and more shed time....

  3. #3
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,657

    Default

    Yep it's called metal stitching it is one of art's that is disappearing I have seen cylinder heads and blocks run for a life time after being repaired in this way, can be performed in place in many cases with disassembly

Similar Threads

  1. Cast Iron Repair
    By Scott in forum WELDING
    Replies: 6
    Last Post: 18th Sep 2013, 01:42 PM
  2. Cast iron pot repair
    By lordnelson in forum METALWORK GENERAL
    Replies: 19
    Last Post: 12th Oct 2011, 08:36 PM
  3. Cast iron table repair
    By neksmerj in forum METALWORK GENERAL
    Replies: 14
    Last Post: 22nd Jun 2011, 07:18 PM
  4. Cast Iron Weld Repair
    By Woodlee in forum WELDING
    Replies: 4
    Last Post: 22nd Jun 2008, 10:13 PM
  5. Repair of Broken Cast Iron
    By Grahame Collins in forum METALWORK GENERAL
    Replies: 0
    Last Post: 11th Feb 2006, 11:35 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •