4th Aug 2016, 10:39 AM #1Senior Member
- Join Date
- Dec 2015
- Location
- Melbourne
- Posts
- 202
Wheel Restoration
I picked up these wheels of ebay the other month for my GT40project. This was one of the ebayphotos, so they obviously needed some work. I drove from Melbourne to Sydney topick them up and have had them in my shed for a little bit.
They were originally on an old XA Landowner FalconCoupe. So could be a few years old.
The centres should be fine, will clean up nicely with somesand blasting/paint stripper/wire brush and re paint.
The problem I have is the outer sections of the 3 piecewheel. These will un bolt and I can workon them separately.
The outers were originally chromed but have quite a bit ofrust starting to show through. Where youcan see the colour change on the outer rim is actually silver paint! See the over spray on the tyre
What would you do, can these be painted over, can I get themre chromed, powder coated?
I have never had to deal with this type of problem.
Cheers.
Ryan
-
4th Aug 2016, 04:19 PM #2Member
- Join Date
- May 2012
- Location
- Oakleigh, Victoria
- Posts
- 55
Lot's of options there,
Sandblast the chrome off them and have them re-plated.
Are the rim sections Steel? You could have them remade in aluminium if you're keen, that way you could get precisely the width and offset you want.
Ceramic coating or powder coating works too although with powder coating you need to need to not coat the mating faces. Metalic powder coats look pretty ordinary. Silver ceramic is pretty shiny and there's a place just around the corner from you that'll do it, Modern Plating.
For a GT40 I'd probably try and reduce the unsprung weight as much as possible and go with aluminium outers. Whitehorse Industries are your friends if you want to head down that path.
-
4th Aug 2016, 04:55 PM #3Senior Member
- Join Date
- Dec 2015
- Location
- Melbourne
- Posts
- 202
A mate has just had some rim half’s spun up from Whitehorse. These were for 18” x 10.5” fronts and they were done in 5mm thick aluminium due to the size of the barrels. The existing rims are probably 2 or 3mm steel. I can’t see a drastic weight saving from going to an aluminium rim, just lots of extra cost say $800. I’m not that fond of these wheels, but they will do for now and I was just looking to neaten them up a little. Long term I would like to get something different.
So just looking at getting some paint on them a suppose.
-
4th Aug 2016, 06:45 PM #4Member
- Join Date
- May 2012
- Location
- Oakleigh, Victoria
- Posts
- 55
Painting would be easy, sand them up and fill the rusty bits. Use an etch primer to stick to the remaining chrome. Apply you choice of colour -Job done. There's plenty of nice silver metalics to choose from.
Not worth over investing if they're not your ideal wheel choice.
You'd probably save at least 5kg per wheel if you went aluminium, those steel rims are heavy. I found 9kg per wheel going from steel wheels to alloy wheels. For a road going car though durability might be the objective rather than minimum weight.
-
4th Aug 2016, 09:32 PM #5Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,942
Ryan, if you are intending to re chrome them, they will need to be highly polished, any marks will show up dramatically. I'd tidy up the centres and paint the rims in a similar colour to the car, parts of the centre where the wheel nuts are could be painted a matching or other colour, to give a distinctive look to them.
KrynTo grow old is mandatory, growing up is optional.
Similar Threads
-
Steering Wheel Restoration
By Goggomobile in forum AUTO RESTORATIONReplies: 8Last Post: 30th Aug 2021, 12:32 AM -
AR Restoration
By Tinkerer77 in forum THE HERCUS AREAReplies: 21Last Post: 16th May 2016, 02:10 PM -
17 Leblond restoration?
By Ueee in forum METALWORK GENERALReplies: 87Last Post: 29th Sep 2014, 11:39 AM -
Thread Restoration
By Anorak Bob in forum METALWORK GENERALReplies: 31Last Post: 30th May 2012, 08:25 PM -
260 restoration
By Finnowa in forum THE HERCUS AREAReplies: 7Last Post: 18th Oct 2010, 12:14 AM