    Hi All, I have a friend who managed to remove some bluing from the side of his barrel with some overzealous cleaning.

    Is re bluing , cold bluing , something the average Joe can tackle? or can you recommend someone who can do it for a reasonable price in Melbourne.

    Assuming the whole barrel would need to be stripped and redone.


    Thanks
    Joe

  2. #2
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    4,594

    Default

    Its not rocket science ,but I somethink some manufactures are free and loose with the truth.

    Here a comparison between well known US brands.

    https://www.huntingnet.com/forum/gun...ts-w-pics.html


    Grahame

  3. #3
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    753

    Default

    In my experience cold blue is just a patch up method, I have never used or heard of one that even comes close to hot blue, in saying that you may only want to
    patch it up, hot blue requires a complete disassembly of the firearm, the last one I had done was about $300

  4. #4
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    4,574

    Default

    Thanks for the lead on that article Grahame.

    The testing suggested the best bluing agent was Nu-Blu from Stock Docs.
    https://stockdocusa.com/shop?olsPage=products
    They still recommend a clear protective coating on top of the bluing called Barricade.

    As it so happens my bro and I were discussing this last weekend and how he wanted to blue some things and I said I would look into it.

    I decided to just try placing a "pretend' order for Nu Blu just to see what the shipping would be.
    Shipping to the US continental states is free but shipping form the US to Oz has become horribly expensive in the last year or so I wanted to see what it was.
    Any way a message comes up “your shipping is free”! I suspect they algorithm that assesses shipping saw WA [Australia] as Washington.
    So I placed an order and it went through with no shipping charge, and have received confirmation about it.

    Now I just went back into look at some other products and a new message has appeared.
    "No international shipping is available at this time. "
    So I'm waiting for the "sorry we cannot ship this" message to come through.

  5. #5
    Join Date
    Dec 2007
    Location
    Adelaide
    Posts
    107

    Default

    I've used cold blue a few times and in my experience while you can coverup small patches you'll find if the patch is any size it will show due to a mismatch in colour - the colour produced by cold blue is actually more of a grey/blue than the deep blue produced by hot nitre blueing.

  6. #6
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    4,574

    Default

    Quote Originally Posted by BobL View Post
    . . . . .Now I just went back into look at some other products and a new message has appeared.
    "No international shipping is available at this time. "
    So I'm waiting for the "sorry we cannot ship this" message to come through.
    Yep email just came through cancelling my order and refunding my payment.

  7. #7
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    4,594

    Default

    We can blame Jerry Harvey for this!

    The net result is that from July 1st , a lot of hobbyists will not be able to obtain certain supplies/ goods - once only available from the overseas source- whether or not the buyer would be willing to pay GST on them, or not.

    The vendors are now deciding, its now all in the too hard basket and we hobbyists are left with no access at all, to those special items we need to make life easier in our respective pursuits.

    It is the same for me as some items in the black powder area of my hobby don't sell enough to warrant keeping them for sale locally and now understandably, the overseas seller does not wish to collect tax for a for a non US government.

    Any further non-gunsmithing comments will need to be placed in the off-topic forum section.

    Grahame

Similar Threads

  1. More metal bluing
    By BobL in forum METALWORK GENERAL
    Replies: 59
    Last Post: 22nd Sep 2018, 11:04 PM
  2. Hot Bluing
    By NedsHead in forum GUNSMITHING
    Replies: 31
    Last Post: 6th Jul 2018, 11:40 PM
  3. Blacking As An Alternative to Bluing
    By Anorak Bob in forum METALWORK GENERAL
    Replies: 7
    Last Post: 6th Jan 2014, 08:32 AM
  4. Bluing
    By bollie7 in forum METALWORK GENERAL
    Replies: 1
    Last Post: 28th Apr 2009, 10:37 PM
  5. Metal bluing solution
    By ohno in forum METALWORK GENERAL
    Replies: 28
    Last Post: 16th Dec 2006, 08:00 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •