    Default Drilling tap a Sportco 33 .222

    I've been asked to drill and tap 2 x M4 through holes on this rifle, about where the small screw and nut are in the crappy photo. I don't want to start unless I know I can do it with a standard HSS drill and tap.
    How hard or tough is the steel?
    Thanks in advance.


  2. #2
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,658

    Default

    HSS should be fine, I have lost count how many I have drilled over the years all with HSS

  3. #3
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    I have a friend who does gunsmith work and he uses spiral taps exclusively on tapped holes for receiver mounted scopes and the like.

    I tried spiral taps and they reduce the tapping effort effort by a big factor.They were dearer but not by a lot.

    Less likely to snap and reduce the chance of an unsuccessful job.

    Grahame

  4. #4
    Join Date
    Feb 2013
    Location
    Laidley, SE Qld
    Posts
    1,039

    Default

    Job's done without any worries, thanks for the advice, the steel was probably as tough as 1045.

Similar Threads

  1. Self drilling taps
    By bob ward in forum METALWORK GENERAL
    Replies: 15
    Last Post: 13th Jul 2015, 08:41 PM
  2. Drilling holes
    By brinesharks in forum METALWORK GENERAL
    Replies: 9
    Last Post: 29th Nov 2009, 03:33 PM
  3. Pre-drilling
    By funkychicken in forum METALWORK GENERAL
    Replies: 12
    Last Post: 23rd Nov 2009, 10:54 AM
  4. Drilling jig help
    By STEAM in forum METALWORK GENERAL
    Replies: 19
    Last Post: 18th Jun 2009, 10:40 PM
  5. Drilling M2
    By funkychicken in forum METALWORK GENERAL
    Replies: 14
    Last Post: 9th Oct 2008, 12:47 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •