27th Apr 2017, 01:51 AM #2China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
HSS should be fine, I have lost count how many I have drilled over the years all with HSS
-
14th May 2017, 04:03 PM #3
I have a friend who does gunsmith work and he uses spiral taps exclusively on tapped holes for receiver mounted scopes and the like.
I tried spiral taps and they reduce the tapping effort effort by a big factor.They were dearer but not by a lot.
Less likely to snap and reduce the chance of an unsuccessful job.
Grahame
-
19th May 2017, 07:31 PM #4Diamond Member
- Join Date
- Feb 2013
- Location
- Laidley, SE Qld
- Posts
- 1,039
Job's done without any worries, thanks for the advice, the steel was probably as tough as 1045.
Similar Threads
-
Self drilling taps
By bob ward in forum METALWORK GENERALReplies: 15Last Post: 13th Jul 2015, 08:41 PM -
Drilling holes
By brinesharks in forum METALWORK GENERALReplies: 9Last Post: 29th Nov 2009, 03:33 PM -
Pre-drilling
By funkychicken in forum METALWORK GENERALReplies: 12Last Post: 23rd Nov 2009, 10:54 AM -
Drilling jig help
By STEAM in forum METALWORK GENERALReplies: 19Last Post: 18th Jun 2009, 10:40 PM -
Drilling M2
By funkychicken in forum METALWORK GENERALReplies: 14Last Post: 9th Oct 2008, 12:47 AM