Thanks: 0
Likes: 0
Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 6 of 6
Thread: Modern Damascus Barrels
-
9th Apr 2016, 12:02 PM #1Member
- Join Date
- Feb 2013
- Location
- Picton NSW
- Posts
- 82
Modern Damascus Barrels
I held the first piece of raw Damasteel Damascus gun barrel material ever sold into Australia the other day.
I am so looking forward to seeing it made into a barrel.
Damasteel Gun Barrel steel Damascus for Custom Firearms DS92xâ„¢/DS96xâ„¢ - Artisan Supplies
hopefully I will be allowed to post pictures as the build progresses. It is the same material used by Purdy in their super expensive Damascus range.
-
9th Apr 2016, 12:53 PM #2
Interesting that a material that the method of making was lost long before guns were invented, is now used to make them. It is a modern approximation of Damascus Steel.
It is still a beautiful material tho. I will be looking forward to seeing any pictures. What method will be used to form the barrel?
Dean
-
9th Apr 2016, 06:29 PM #3
I met one of the gun smiths from Purdy the other day. I bought some machines from him he was clearing out an estate. Included in what I bought was a power Hacksaw which he was using to cut up antique Damascus shot gun barrels before I could take the saw.
Funny coincidence…..Live a Quiet Life & Work with your Hands
-
10th Apr 2016, 03:34 PM #4
Hi Dean
there's a book called 'Out of the Fiery Furnace" which among many many other things covers the disappearance of Damascus steel. The method of making Damascus steel wasn't so much lost as bypassed. All early steels were hammer forged and their properties depended more on the impurities (what today are known as alloying elements) contained within the local source of iron and charcoal.
From what I recall, Damascus steel disappeared around the time England's iron making industry started exporting cheap iron ingots. The Damascus smiths switched to the cheaper supply and the rest is history as they say ...regards from Canmore
ian
-
10th Apr 2016, 10:01 PM #5
My memory must be going, going gone.
You are right. It was not the method so much as the exact ingredients, although the precise method had been lost. Of course just because I read it does not mean it is correct. Ancient history as you said. The only benefit is its historical value and appearance.
Dean
-
12th Apr 2016, 01:52 AM #6China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,657
Who is going to make the barrel
Similar Threads
-
Cable Damascus
By DSEL74 in forum THE SMITHYReplies: 9Last Post: 17th Dec 2015, 08:11 PM -
Modern Toolmaking Methods - A Treatise by Franklin D. Jones
By morrisman in forum METALWORK GENERALReplies: 3Last Post: 7th Jun 2012, 01:42 AM -
Damascus/ironwood knife
By ohno in forum KNIFE MAKINGReplies: 25Last Post: 18th Nov 2006, 11:17 AM -
Hydrochloric acid for Damascus?
By ohno in forum METALWORK GENERALReplies: 10Last Post: 10th Oct 2006, 09:49 PM