    Default Modern Damascus Barrels

    I held the first piece of raw Damasteel Damascus gun barrel material ever sold into Australia the other day.
    I am so looking forward to seeing it made into a barrel.
    Damasteel Gun Barrel steel Damascus for Custom Firearms DS92x™/DS96x™ - Artisan Supplies

    hopefully I will be allowed to post pictures as the build progresses. It is the same material used by Purdy in their super expensive Damascus range.

  2. #2
    Join Date
    Jan 2011
    Location
    Far West Wimmera
    Age
    58
    Posts
    4,088

    Default

    Interesting that a material that the method of making was lost long before guns were invented, is now used to make them. It is a modern approximation of Damascus Steel.

    It is still a beautiful material tho. I will be looking forward to seeing any pictures. What method will be used to form the barrel?

    Dean

  3. #3
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,527

    Default

    I met one of the gun smiths from Purdy the other day. I bought some machines from him he was clearing out an estate. Included in what I bought was a power Hacksaw which he was using to cut up antique Damascus shot gun barrels before I could take the saw.

    Funny coincidence
    ..Live a Quiet Life & Work with your Hands

  4. #4
    Join Date
    Feb 2003
    Location
    formerly from Sydney (north of The Harbour), NSW, Oz
    Age
    63
    Posts
    289

    Default

    Quote Originally Posted by Oldneweng View Post
    Interesting that a material that the method of making was lost long before guns were invented, is now used to make them. It is a modern approximation of Damascus Steel.
    Hi Dean

    there's a book called 'Out of the Fiery Furnace" which among many many other things covers the disappearance of Damascus steel. The method of making Damascus steel wasn't so much lost as bypassed. All early steels were hammer forged and their properties depended more on the impurities (what today are known as alloying elements) contained within the local source of iron and charcoal.

    From what I recall, Damascus steel disappeared around the time England's iron making industry started exporting cheap iron ingots. The Damascus smiths switched to the cheaper supply and the rest is history as they say ...
    regards from Canmore

    ian

  5. #5
    Join Date
    Jan 2011
    Location
    Far West Wimmera
    Age
    58
    Posts
    4,088

    Default

    Quote Originally Posted by ian View Post
    Hi Dean

    there's a book called 'Out of the Fiery Furnace" which among many many other things covers the disappearance of Damascus steel. The method of making Damascus steel wasn't so much lost as bypassed. All early steels were hammer forged and their properties depended more on the impurities (what today are known as alloying elements) contained within the local source of iron and charcoal.

    From what I recall, Damascus steel disappeared around the time England's iron making industry started exporting cheap iron ingots. The Damascus smiths switched to the cheaper supply and the rest is history as they say ...
    My memory must be going, going gone.

    You are right. It was not the method so much as the exact ingredients, although the precise method had been lost. Of course just because I read it does not mean it is correct. Ancient history as you said. The only benefit is its historical value and appearance.

    Dean

  6. #6
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    811

    Default

    Who is going to make the barrel

Similar Threads

  1. Cable Damascus
    By DSEL74 in forum THE SMITHY
    Replies: 9
    Last Post: 17th Dec 2015, 08:11 PM
  2. Modern Toolmaking Methods - A Treatise by Franklin D. Jones
    By morrisman in forum METALWORK GENERAL
    Replies: 3
    Last Post: 7th Jun 2012, 01:42 AM
  3. Damascus/ironwood knife
    By ohno in forum METALWORK GENERAL
    Replies: 25
    Last Post: 18th Nov 2006, 11:17 AM
  4. Hydrochloric acid for Damascus?
    By ohno in forum METALWORK GENERAL
    Replies: 10
    Last Post: 10th Oct 2006, 09:49 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •