    Default Casting Anvils

    I started this journey with making a small wooden split pattern but couldnít figured a good way to do my logo and the text. Sometime later I got a Aldi 3D Printer.

    So I downloaded Fusion 360 and got to learning on the fly and 3D modeled my anvil with draft.


    First print using sample filament that came with the printer hence color changes as it ran out.




    I printed a whole bunch more for economics itís cheaper to have 8 in a mould than individually ram each one up.

    Had a fixed flask dimension and had to try to work out how many I could fit into the flask and where the sprue, runners, gates etc would be.



    I sprayed all the prints with high build spray putty and hand sanded them all back with wet n dry paper. I didnít want any of the print layers showing through.




    I drew up a template for the flask and drilled the location pins.



    The match plate all rammed up gives this sand mould in the flask.


    After pouring in bronze.

    Ö..Live a Quiet Life & Work with your Hands

  2. #2
    Join Date
    Dec 2011
    Location
    Sydney
    Posts
    234

    Default

    Congratulations!
    A great demo of design to print to casting. What metal?
    Cheers
    Bill

  3. #3
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,519

    Default

    Damn ivíe lost the second post.


    I did Bronze, Brass, and SG Iron.
    Ö..Live a Quiet Life & Work with your Hands

  4. #4
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,519

    Default

    The next step was a side step as I had to rebuild the mill to finish the anvils. That can be seen in another thread.


    Basic clean up of the flashing. 24 Minis, 8 of each Metal.



    Milled the base and then the tops.



    Followed this up with some wire wheeling, filing, and a scotch brute fine wheel.

    20 finished, the 4 remaining will be kept to pass on to my Daughter.


    These were meant to go on to my market stall this weekend at Yarra Glen. But I have nearly sold out in one day I have 1 SG Iron, 2 Bronze and 5 Brass left. Thatís what I get for showing them on Facebook.

    Some even went to collectors in USA and Australia. Allocating anvils to orders and packaging and posting.
    Ö..Live a Quiet Life & Work with your Hands

  5. #5
    Join Date
    Jan 2007
    Location
    Dee Why NSW
    Posts
    158

    Default

    Very nice. Out of interest, what are they selling for?
    Built: a Bench,a Desk,an Archery Display,

    Those were the droids I was looking for.

  6. #6
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,519

    Default

    $60ea for Brass & SG Iron, $70 Bronze.
    Ö..Live a Quiet Life & Work with your Hands

  7. #7
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    3,502

    Default

    beautiful work DSEL

  8. #8
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    733

    Default

    Can I have the SG posted to SA at my cost

  9. #9
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,519

    Default

    Quote Originally Posted by China View Post
    That is great read, so how long do I have to wait for the net lot 1 brass and one SG
    Iíve got 1 SG left and 5 Brass
    Send me a PM if you want them
    Ö..Live a Quiet Life & Work with your Hands

Similar Threads

  1. Anvils
    By Bob47 in forum THE SMITHY
    Replies: 8
    Last Post: 27th Feb 2013, 07:26 PM
  2. Anvils?
    By Aerohydro in forum THE SMITHY
    Replies: 36
    Last Post: 11th Nov 2012, 11:16 PM
  3. Casting about for cast iron casting ideas
    By Graziano in forum THE FOUNDRY
    Replies: 49
    Last Post: 1st Apr 2012, 12:05 PM
  4. Anvils for sale- SE Qld.
    By Andy Mac in forum METALWORK GENERAL
    Replies: 0
    Last Post: 25th Oct 2008, 12:45 PM
  5. Anvils
    By Marc in forum METALWORK GENERAL
    Replies: 2
    Last Post: 28th Sep 2007, 06:38 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •