Thread: KEG Foundry Furnace biuld
-
8th Jul 2018, 08:00 PM #1
KEG Foundry Furnace biuld
I started this KEG Foundry Furnace project a few years ago and now have some time to finish it off . I had two old beer kegs lying around so why not put them to use. Been researching DIY Foundry Furnaces and came across the (myfordboy) web site, So will be building a oil burner like he has built.
Resize of IMG_5410.jpgResize of IMG_5409.jpgResize of IMG_5506.jpgResize of IMG_5522.jpgResize of IMG_5519.jpgResize of IMG_5824.jpgResize of IMG_5823.jpg
-
8th Jul 2018, 08:15 PM #2
Poured in the refractory cement into the lid and the bottom of the keg, will line the side of the keg with fire bricks.
Resize of IMG_6323.jpgResize of IMG_6338.jpg
-
9th Jul 2018, 03:53 AM #3Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,671
Been planning to build a keg-based furnace myself, so watching with interest.
Where did you get your refractory materials from?
Steve
-
9th Jul 2018, 05:49 AM #4
-
9th Jul 2018, 06:11 AM #5
Got some work done on the supply station, i had to make a stronger base as 60 litters of oil and 25 litters in the top tank was to heavy and with those small caster wheels the hole thing could tip over. I hack a PC power supply for the 12 volt oil pump witch will top up the top tank,don't want to run out of oil when doing a melting season. I'm using 135 micron mesh for filtering WASTE VEGETABLE OIL.
Resize of IMG_5515.jpgResize of IMG_5512.jpgResize of IMG_6185.jpgResize of IMG_6183.jpgResize of IMG_6184.jpg
-
10th Jul 2018, 09:48 PM #6
Here are some photos of the oil burner, the veg oil needs to be heated up a bit so it's easy to lite. A couple of vids of test runs. https://www.youtube.com/watch?v=rqDcboE___Q https://www.youtube.com/watch?v=nN6Rf-LuhsQ
Resize of IMG_6193.jpgResize of IMG_6194.jpgResize of IMG_6195.jpgResize of IMG_6196.jpgResize of IMG_6197.jpgResize of IMG_6198.jpg
-
29th Jul 2018, 05:04 PM #7
Today i cut the hole for the tuyere and use a propane torch to slowly heat the furnace up to ~400c, next week will use the oil burner. The refractory has been drying for about 7 months so just want to make sure there is no moisture left before i cerment the fire bricks in.
Resize of IMG_6824.jpgResize of IMG_6825.jpgResize of IMG_6826.jpgResize of IMG_6828.jpgResize of IMG_6827.jpg
-
17th Aug 2018, 06:28 PM #8
I cut up the fire bricks to the required size for the keg and used high temp cement to hold the bricks in, i ran out out of high temp cement will get some more to finish off and trim the top off with a hand saw.
Resize of IMG_6861.jpgResize of IMG_6864.jpgResize of IMG_6863.jpg
-
21st Aug 2018, 06:33 PM #9Diamond Member
- Join Date
- Aug 2006
- Location
- Melbourne
- Posts
- 1,106
What high temp cement are you using and where do you get it from?
I also like your oil burner, do you have much $$$ invested in it?
Thanks
-
21st Aug 2018, 07:39 PM #10
I got the cement from Refractory and Ceramic PTY LTD in Mulgrave Vic So far the cost is $1,000 and counting. I found out Bunnings are selling High Temperature Mortar Heat resistant up to 1000°C will need to get some to finish off the brick work.
Resize of IMG_6860.jpgResize of IMG_6859.jpg
-
27th Aug 2018, 02:07 PM #11
Got the high temp mortar and finish off the brick work and had plenty left over, so applied the rest on the inside and top. I have a 8 inch stainless tube which i would like to use for a test melt. There is 1 inch gap between the tube and the wall of the furnace, would the gap be OK?
Resize of IMG_6866.jpgResize of IMG_6867.jpgResize of IMG_6869.jpgResize of IMG_6870.jpg
-
31st Aug 2018, 01:51 PM #12I break stuff...
- Join Date
- Aug 2010
- Location
- Toorloo Arm, VIC
- Age
- 39
- Posts
- 1,298
Interesting.... I've had a keg kicking around for years. Always thought it was aluminium for some reason, but I'm going to have to re-check now. But ouch on the price so far - how much of that was the burner, and how much the refractory?
-
31st Aug 2018, 03:56 PM #13
-
10th Apr 2019, 06:25 PM #14Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Similar Threads
-
Foundry Myths
By RayG in forum THE FOUNDRYReplies: 11Last Post: 19th Nov 2021, 09:48 PM -
foundry sand
By texx in forum METALWORK - Machinery, Equipment, MARKETReplies: 0Last Post: 20th Oct 2016, 12:05 PM -
Furnace kit
By AndrewOC in forum EBAY, GUMTREE, and other off forum sales sitesReplies: 0Last Post: 28th Apr 2015, 12:29 PM -
The Charcoal Foundry
By silentC in forum THE FOUNDRYReplies: 63Last Post: 5th Sep 2009, 10:44 PM -
Backyard Foundry
By InkSpot in forum METALWORK GENERALReplies: 3Last Post: 10th Feb 2008, 07:40 PM