    Default Ceramic fiber rigidizer, where to buy?

    Hi all,

    Just wondering where would be the best place to source some Ceramic fiber rigidizer for sealing ceramic fiber blanket? I contacted a few places already but they only had 20 litre containers of it available. I am only after about 1 or 2 litres. I think it has a shelf life, 12 months maybe, so 20 litres would be far too much.

    I'm in Melbourne, south east suburbs so somewhere around there would be good.

    Thanks

  2. #2
    Join Date
    Dec 2005
    Location
    Canberra
    Posts
    490

    Default

    A possibility is that you could use sodium silicate as it will do that sort of job.

    You can get it ready made from a pottery place (about $12/litre) or you can make your own using kitty litter and caustic soda (videos of this on YouTube) for about $3/litre. (200 grams caustic soda, 300 grams silica gel kitty litter, 500ml water).

  3. #3
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by Master Splinter View Post
    A possibility is that you could use sodium silicate as it will do that sort of job.

    You can get it ready made from a pottery place (about $12/litre) or you can make your own using kitty litter and caustic soda (videos of this on YouTube) for about $3/litre. (200 grams caustic soda, 300 grams silica gel kitty litter, 500ml water).
    200g of caustic in 300g of Silica seems like a lot of caustic, or maybe that much is needed to dissolve the silica jell kitty litter?

    The rigidizer I have has a pH of 11 which means it is alkaline but not as much as I would have thought that 200g or caustic per litre would produce.
    One MSDS sheets I have seen for rigidizer claimed it only contained about 1% Na2O.

    Some MSDS sheets don't mention any caustic, just 30-50% amorphous silica and some mention <10% ethylene glycol.
    I assume the EG is a stabiliser for the soluble silica?.

    My understanding of rigidizer is enough amorphous silica is needed between the kaowool fibres so that when the kiln is fired the amorphous silica partially melts the fibres together.
    Sodium may be added to reduce the melting point of the silica in between the fibres because pure Si doesn't melt until about 1600º?
    However there may enough free Na around on the fibres for the binding to take place anyway.

  4. #4
    Join Date
    Jan 2016
    Location
    Wodonga Vic
    Age
    38
    Posts
    633

    Default

    The chemical reaction to form sodium silicate is one part SiO2 to two parts NaOH, that works out to be 60.08 grams of silica gel kitty litter (assuming it's pure silicon dioxide) for every 79.994 grams of caustic soda, however I would add a little excess of silica gel (say 5-10 grams) to insure all of the caustic soda has been used up in the reaction.

    if you're going to make your own sodium silicate use a stainless steel bowl, hot caustic soda will eat through glass

  5. #5
    Ueee's Avatar
    Ueee is offline Blacksmith, Cabinetmaker, Machinist, Messmaker
    Join Date
    Dec 2011
    Location
    Canberra
    Age
    40
    Posts
    4,515

    Default

    You could ask Brett Selley or Gameco, Gameco sell his refactory kits which include a small amount of the rigidizer. Brett can be contacted through the ABF.
    I would highly recommend putting a hardface over the blanket as well, there are many products suitable, i just use satanite. The blanket is an excellent insulator but the hardface reflects heat very well. It also makes for a more durable and easily repairable surface.
    1915 17"x50" LeBlond heavy duty Lathe, 24" Queen city shaper, 1970's G Vernier FV.3.TO Universal Mill, 1958 Blohm HFS 6 surface grinder, 1942 Rivett 715 Lathe, 14"x40" Antrac Lathe, Startrite H225 Bandsaw, 1949 Hercus Camelback Drill press, 1947 Holbrook C10 Lathe.

  6. #6
    Join Date
    Aug 2006
    Location
    Melbourne
    Posts
    1,106

    Default

    Will try and make some sodium silicate, seems easy enough to do. Though it seems I can only find 98% sodium hydroxide. Is this going to work? https://www.bunnings.com.au/diggers-...-soda_p1560250

    With the Satanite refractory will it last if I were to purchase the large 24kg bag or does it have a use by date?

    Is there any other hard face alternatives, is there a diy version of it out there?


    Thanks

  7. #7
    Join Date
    Jan 2016
    Location
    Wodonga Vic
    Age
    38
    Posts
    633

    Default

    Yeah that's fine Com_VC, you'll never get perfectly dry sodium hydroxide, it's hygroscopic and always has at least a few % water, what you don't want is aluminium added to it, I've checked the MSDS and the Diggers brand looks fine, it's even suitable for soap making, here it is in pdf, http://www.recochem.com.au/files/dow...Soda_Mar15.pdf

Similar Threads

  1. re ceramic blanket
    By texx in forum THE FOUNDRY
    Replies: 11
    Last Post: 5th Sep 2013, 10:47 PM
  2. Do you lubricate Ceramic bearings
    By rodm in forum METALWORK GENERAL
    Replies: 2
    Last Post: 9th Dec 2010, 10:26 AM
  3. Source of Ceramic Wool OR Kiln Bricks
    By thumbsucker in forum METALWORK GENERAL
    Replies: 12
    Last Post: 2nd Sep 2008, 07:48 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •